The filtration of large grey and ductile iron castings

نویسنده

  • E. Wiese
چکیده

Filtration of mass produced automobile castings is widely and successful applied, less common and more difficult is the filtration of large castings heavier than 1.000 kg. The paper deals with the special problems of applying filtration to such castings including; filter selection, description of three special filtration gating system concepts, along with ten case studies are given.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A review on fatigue design of heavy section EN-GJS-400-18-LT ductile iron wind turbine castings

A comprehensive review of fatigue behavior and fatigue design of heavy section wind turbine castings made of ductile iron EN-GJS-400-18-LT is performed. Common metallurgical defects that are affecting fatigue behavior of this material were studied. Review of different researches on quantitative effect of chunky graphite and micro structure on fatigue behavior of EN-GJS-400-18-LT was perform...

متن کامل

Effect of Melting Techniques on Ductile Iron Castings Properties

Ductile iron is one of the most important engineering materials, in view of its excellent castability, signifi cantly better mechanical properties and low cost [1, 2]. It represents the fastest growing segment of the iron market. In the medium term, it is to be expected that the market share of nodular iron will level off at 40 % to 45 % [3]. Achieving the full potential of ductile iron require...

متن کامل

Analyzing the Failure of Master Mould in Casting of Copper Anode Moulds and Suggesting a more Suitable Metal Mould

Master moulds are used to cast copper anode moulds. These iron moulds are made of grey or nodular cast irons. According to desirable properties of ductile irons, it was expected that ductile cast iron ...

متن کامل

Literature search - Deteriorated Graphite Structures on Cast Iron Skins

The fatigue strength offerritic ductile iron, Grade EN-GJS-400-18U-LT. was determined for large section castings measuring 4 by 24 by 24 inches. Fatigue testing was conducted in bending fatigue in order to determine the influence of surface conditions on fatigue strength. Test specimens with various surface conditions were evaluated, including notched and un-notched specimens, as well as those ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2006