BACKGROUND This study aimed to investigate the microshear bond strength of universal bonding adhesives to leucite-reinforced glass-ceramic. METHODS Leucite-reinforced glass-ceramic blocks were polished and etched with 9.5% hydrofluoric acid for 1 min. The specimens were assigned to one of four groups based on their surface conditioning (n = 16): 1) NC: negative control with no further treatment; 2) SBU: Single Bond Universal (3M ESPE); 3) ABU: ALL-BOND Universal (Bisco); and 4) PC: RelyX Ceramic Primer and Adper Scotchbond Multi-Purpose Adhesive (3M ESPE) as a positive control. RelyX Ultimate resin cement (3M ESPE) was placed on the pretreated ceramic and was light cured. Eight specimens from each group were stored in water for 24 h, and the remaining eight specimens were thermocycled 10,000 times prior to microshear bond strength evaluation. The fractured surfaces were examined by stereomicroscopy and scanning electron microscopy (SEM). RESULTS After water storage and thermocycling, the microshear bond strength values decreased in the order of PC > SBU and ABU > NC (P < 0.05). Thermocycling significantly reduced the microshear bond strength, regardless of the surface conditioning used (P < 0.05). Cohesive failure in the ceramic and mixed failure in the ceramic and resin cement were observed in the fractured specimens. The percentage of specimens with cohesive failure after 24 h of water storage was: NC (50%), SBU (75%), ABU (75%), and PC (87%). After thermocycling, the percentage of cohesive failure in NC decreased to 25%; however, yet the percentages of the other groups remained the same. CONCLUSIONS Although the bond strength between resin and hydrofluoric acid-etched glass ceramic was improved when universal adhesives were used, conventional surface conditioning using a separate silane and adhesive is preferable to a simplified procedure that uses only a universal adhesive for cementation of leucite-reinforced glass-ceramic.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Laboratory Performance of Universal Adhesive Systems for Luting CAD/CAM Restorative Materials.

PURPOSE To evaluate the microshear bond strength (μSBS) of several universal adhesive systems applied on five different indirect restorative materials. MATERIALS AND METHODS Five CAD/CAM materials were selected: 1) indirect resin composite (LAV); 2) feldspathic glass ceramic (VTR); 3) leucite-reinforced glass-ceramic (EMP); 4) lithium disilicate ceramic (EMX); 5) yttrium-stabilized zirconium ...

متن کامل

The effect of silane applied to glass ceramics on surface structure and bonding strength at different temperatures

PURPOSE To evaluate the effect of various surface treatments on the surface structure and shear bond strength (SBS) of different ceramics. MATERIALS AND METHODS 288 specimens (lithium-disilicate, leucite-reinforced, and glass infiltrated zirconia) were first divided into two groups according to the resin cement used, and were later divided into four groups according to the given surface treat...

متن کامل

Six-Year Results of Leucite- Reinforced Glass Ceramic Crowns

A leucite-reinforced glass ceramic material (IPS-Empress) was developed for clinical use in Zurich. A prospective clinical study of these laboratory-made all-ceramic crowns revealed encouraging result with an estimated 2-year survival rate of 95%. The aim of the present study was to determine the clinical behavior during a longer period of observation with respect to a possible fatigue fracture...

متن کامل

Influence of surface conditioning on ceramic microstructure and bracket adhesion.

The objective of this study was to investigate the influence of different conditioning procedures on various ceramic microstructures and bracket adhesion. Ceramic specimens (feldspathic, leucite, leucite-free, and fluorapatite) were mechanically conditioned (n = 20 per ceramic type) with conventional hydrofluoric acid (5 per cent HF; 60/30 seconds), buffered hydrofluoric acid (9.6 per cent BHF;...

متن کامل

Analysis of Self-Adhesive Resin Cement Microshear Bond Strength on Leucite-Reinforced Glass-Ceramic with/without Pure Silane Primer or Universal Adhesive Surface Treatment

OBJECTIVE To evaluate the microshear bond strength (μSBS) of self-adhesive resin (SA) cement on leucite-reinforced glass-ceramic using silane or universal adhesive. MATERIALS AND METHODS Ceramic blocks were etched with 9.5% hydrofluoric acid and divided into three groups (n = 16): (1) negative control (NC) without treatment; (2) Single Bond Universal (SBU); (3) RelyX Ceramic Primer as positiv...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 19  شماره 

صفحات  -

تاریخ انتشار 2015