The Contact Ageing Effect on Fretting Damage of an Electro-Deposited Coating against an AISI52100 Steel Ball

نویسندگان

  • Kyungmok Kim
  • Joon Soo Ko
چکیده

This article investigates the effect of contact ageing on fretting damage of an epoxy-based cathodic electro-deposited coating for use on automotive seat slide tracks (made of cold-rolled high strength steel). Static normal load was induced at the contact between the coating and an AISI52100 ball for a certain duration. It was identified that plastically deformed contact area increased logarithmically as a function of time when the contact was under static normal load. Fretting tests after various durations of static contact were conducted using a ball-on-flat plate apparatus. All fretting tests were halted when the friction coefficient reached a critical value of 0.5, indicating complete coating failure. The total number of fretting cycles to the critical friction coefficient was found to vary with the duration of static contact before fretting. It was identified that the number of cycles to the critical friction coefficient decreased with the increased duration of static contact. Meanwhile, the friction coefficient at steady-state sliding was not greatly affected by the duration of static contact before fretting. Finally, the relation between coating thickness after indentation creep and the number of cycles to the critical friction coefficient was found to be linear. Obtained results show that the duration of static contact before fretting has an influence on the fretting lifetime of an electro-deposited coating.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Statistical Determination of a Fretting-Induced Failure of an Electro-Deposited Coating

This paper describes statistical determination of fretting-induced failure of an electro-deposited coating. A fretting test is conducted using a ball-on-flat plate configuration. During a test, a frictional force is measured, along with the relative displacement between an AISI52100 ball and a coated flat specimen. Measured data are analyzed with statistical process control tools; a frictional ...

متن کامل

Evaluation and Description of Friction between an Electro-Deposited Coating and a Ceramic Ball under Fretting Condition

This article describes fretting behavior of zirconia and silicon nitride balls on an electro-deposited coating. Fretting tests are performed using a ball-on-flat configuration. The evolution of the kinetic friction coefficient is determined, along with slip ratio. Experimental results show that the steady-state friction coefficient between ceramic balls (Si₃N₄ and ZrO₂) and an electro-deposited...

متن کامل

Enhanced Anti-corrosive Properties of Electrosynthesized Polyaniline/zeolite Nanocomposite Coatings on Steel

The preparation of polyaniline/zeolite nanocomposite coating on 304 stainless steel (304 SS) surface has studied via the galvanostatic method. The electro-generated coating was characterized by Fourier transform infrared spectroscopy (FT-IR), UV-visible absorption spectroscopy, X-ray diffraction (XRD) patterns and scanning electron microscopy (SEM). The anticorrosion property of polyaniline/zeo...

متن کامل

Shot Peening as an Alternative to Fatigue Life Improvement of CK45 Steel Coated with an Electroless Ni-Cu-P

The effect of an electroless Ni-Cu-P coating on the fatigue behavior of quenched and tempered CK45 steel has been investigated. The fatigue tests under rotating bending conditions have been conducted in three different conditions of uncoated, as-deposited and shot peened prior to the coating deposition. The results indicate that plating of the base steel leads to a fatigue life reduction. The d...

متن کامل

Self-Cleaning Properties of TiN/CrN Nanoscale Multi-layer Deposited on Surgical 420C Stainless Steel

The present paper focuses on the investigation of self-cleaning properties based on studding of water repellency and blood repellency for TiN- and CrN single-layer and TiN/CrN nanoscale multi-layer coatings deposited via Cathodic Arc Evaporation (CAE) method on medical grade 420C stainless steel substrate. X-ray diffraction (XRD) method and Field Emission Scanning Electron Microscope (FESEM) wa...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 9  شماره 

صفحات  -

تاریخ انتشار 2016