In Vitro assessment of dentin erosion after immersion in acidic beverages: surface profile analysis and energy-dispersive X-ray fluorescence spectrometry study.

نویسندگان

  • Taciana Marco Ferraz Caneppele
  • Raffaela Di Iorio Jeronymo
  • Rebeca Di Nicoló
  • Maria Amélia Máximo de Araújo
  • Luís Eduardo Silva Soares
چکیده

The aim of this study was to investigate the effects of some acidic drinks on dentin erosion, using methods of surface profile (SP) analysis and energy-dispersive X-ray fluorescence spectrometry (EDXRF). One hundred standardized dentin slabs obtained from bovine incisor roots were used. Dentin slabs measuring 5x5 mm were ground flat, polished and half of each specimen surface was protected with nail polish. For 60 min, the dentin surfaces were immersed in 50 mL of 5 different drinks (Gatorade®, Del Valle Mais orange juice®, Coca-Cola®, Red Bull® and white wine), 20 blocks in each drink. The pH of each beverage was measured. After the erosive challenge, the nail polish was removed and SP was analyzed. The mineral concentration of dentin surfaces was determined by means of EDXRF. Data were analyzed statistically by ANOVA and Tukey's test (α=0.05). SP analysis showed that Red-Bull had the highest erosive potential (p<0.05). EDXRF results exhibited a decrease in phosphate in the groups immersed in Red-Bull, orange juice and white wine (p<0.05), and no significant difference in calcium content between the reference surface and eroded surface. In conclusion, this study demonstrated that all studied beverages promoted erosion on root dentin and Red Bull had the highest erosive potential. There was no correlation between pH of beverages and their erosive potential and only the P content changed after erosive challenge.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fabrication, Characterization and Osteoblast Response of Cobalt-Based Alloy/Nano Bioactive Glass Composites

IIn this work, cobalt-based alloy/ nano bioactive glass (NBG) composites with 10, 15 and 20 wt% NBG were prepared and their bioactivity after immersion in simulated body fluid (SBF) for 1 to 4 weeks was studied. The scanning electron microscopy images of two- step sintered composites revealed a relatively dense microstructure the density of which decreased with the increase in the NBG amount. M...

متن کامل

Heat Treatment Of Cobalt-Base Alloy Surgical Implants With Hydroxyapatite-Bioglass For Surface Bioactivation

ASTM F-75 Cobalt-base alloy castings are widely used for manufacturing orthopedic implants. This alloy needs both homogenization and solutionizing heat treatment after casting, as well as bioactivation of the surface to increase the ability of tissue bonding. In this study, ASTM F-75 Cobalt-base substrate was heat treated at 1220°C for 1 hour in contact with Hydroxyapatite-Bioglass powder in or...

متن کامل

Enhanced bioactive properties of BiodentineTM modified with bioactive glass nanoparticles

Objective To prepare nanocomposite cements based on the incorporation of bioactive glass nanoparticles (nBGs) into BiodentineTM (BD, Septodent, Saint-Maur-des-Fosses Cedex, France) and to assess their bioactive properties. Material and Methods nBGs were synthesised by the sol-gel method. BD nanocomposites (nBG/BD) were prepared with 1 and 2% nBGs by weight; unmodified BD and GC Fuji IX (GIC, ...

متن کامل

A Study on ZnO Nanorod Arrays Formed on the Surface of Polyester Fabric

A feasibility study on the possible growth of rod-shaped nano size zinc oxide particles on the surface of polyester fabric was investigated. The nanoparticles were produced using a hydrolysis method, with a zinc compound being utilized as the starter material. Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy/energy dispersive X-ray spectrometry (SEM/EDS) and X-ray d...

متن کامل

In Vitro Bioactivity Test of Real Dental Implants According to ISO 23317.

PURPOSE The goal of this study was to compare the in vitro bioactivity in simulated body fluid (SBF) of commercially available dental implants. MATERIALS AND METHODS Bioactivity, according to ISO 23317, of commercially available dental implants with various surface modifications (BIO-surface, SLA, SLActive, TiUnite, and OsseoSpeed) was tested in SBF for 1 and 3 weeks. Surface characterization...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Brazilian dental journal

دوره 23 4  شماره 

صفحات  -

تاریخ انتشار 2012