Measurement of the residual stress tensor in a compact tension weld specimen

نویسنده

  • Y. Traore
چکیده

Neutron diffraction measurements have been performed to determine the full residual stress tensor along the expected crack path in an austenitic stainless steel (Esshete 1250) compact tension weld specimen. A destructive slitting method was then implemented on the same specimen to measure the stress intensity factor profile associated with the residual stress field as a function of crack length. Finally deformations of the cut surfaces were measured to determine a contour map of the residual stresses in the specimen prior to the cut. The distributions of transverse residual stress measured by the three techniques are in close agreement. A peak tensile stress in excess of 600 MPa was found to be associated with an electron beam weld used to attach an extension piece to the test sample, which had been extracted from a pipe manual metal arc butt weld. The neutron diffraction measurements show that exceptionally high residual stress triaxiality is present at crack depths likely to be used for creep crack growth testing and where a peak stress intensity factor of 35 MPa√m was measured (crack depth of 21 mm). The neutron diffraction measurements identified maximum values of shear stress in the order of 50 MPa and showed that the principal stress directions were aligned to within ~20° of the specimen orthogonal axes. Furthermore it was confirmed that measurement of strains by neutron diffraction in just the three specimen orthogonal directions would have been sufficient to provide a reasonably accurate characterisation of the stress state in welded CT specimens.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Experimental Study of the Residual Stresses in Girth Weld of Natural Gas Transmission Pipeline

In order to achieve integrated condition in the girth welding of high pressure natural gas transmission pipelines, the weld zones and its surrounding area should have good mechanical properties. Residual stresses are an important defect especially in the girth welding of the pipeline. In this study, two API X70 steel pipes (with spiral seam weld) of 56 inches outside diameter and 0.780 inch wal...

متن کامل

Application of Pulse Method to Incremental Slitting Measurement of Residual Stresses in Laminated Composites

In this research, the incremental slitting method was employed to determine throughthickness residual stress profile of a carbon/epoxy laminate. The method involves measuring strains at the back surface of the stressed specimen, while a narrow slit is cut by a CNC milling machine progressively from the top surface of the specimen. "Pulse Method" was selected as the computational approach for th...

متن کامل

A Study of Residual Stresses and Microstructure in 2024-T3 Aluminum Friction Stir Butt Welds

Three-dimensional residual stress mapping of an aluminum 2024-T3 arcan specimen, butt-welded by the friction stir technique, was performed by neutron diffraction. Results indicate that the residual stress distribution profiles across the weld region are asymmetric with respect to the weld centerline, with the largest gradients in the measured residual stress components occurring on the advancin...

متن کامل

Effect of geometrical variable and welding sequence on residual stresses and deformation in a 5083-H321 aluminum T joint

Studies on welding process of Aluminium weldments shows that post-weld residual stress and deformation are influential on structure efficiency and there are different variable which affect these stresses and deformation. In this study the effect of geometrical variables and welding sequence on residual stresses and deformation in Aluminium H321 have investigated by the finite element software A...

متن کامل

Effect of geometrical variable and welding sequence on residual stresses and deformation in a 5083-H321 aluminum T joint

Studies on welding process of Aluminium weldments shows that post-weld residual stress and deformation are influential on structure efficiency and there are different variable which affect these stresses and deformation. In this study the effect of geometrical variables and welding sequence on residual stresses and deformation in Aluminium H321 have investigated by the finite element software A...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2012