Hydraulic Fracture and Toughening of a Brittle Layer Bonded to a Hydrogel.

نویسندگان

  • Alessandro Lucantonio
  • Giovanni Noselli
  • Xavier Trepat
  • Antonio DeSimone
  • Marino Arroyo
چکیده

Brittle materials propagate opening cracks under tension. When stress increases beyond a critical magnitude, then quasistatic crack propagation becomes unstable. In the presence of several precracks, a brittle material always propagates only the weakest crack, leading to catastrophic failure. Here, we show that all these features of brittle fracture are fundamentally modified when the material susceptible to cracking is bonded to a hydrogel, a common situation in biological tissues. In the presence of the hydrogel, the brittle material can fracture in compression and can hydraulically resist cracking in tension. Furthermore, the poroelastic coupling regularizes the crack dynamics and enhances material toughness by promoting multiple cracking.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Failure Modes in Ceramic-Based Layer Structures: A Basis for Materials Design of Dental Crowns

A research program on failure modes induced by spherical indenters in brittle layer structures bonded to polymeric substrates, in simulation of occlusal function in all-ceramic dental crowns, is surveyed. Tests are made on model flat and curved layers bonded onto a dentin-like polymer base, in bilayer (ceramic/polymer) and trilayer (ceramic/ceramic/polymer) configurations. All-transparent syste...

متن کامل

Fracture and Fatigue Behavior at Ambient and Elevated Temperatures of Alumina Bonded with Copper/Niobium/Copper Interlayers

Interfacial fracture toughness and cyclic fatigue-crack growth properties of joints made from 99.5% pure alumina partially transient liquid-phase bonded using copper/niobium/copper interlayers have been investigated at both room and elevated temperatures, and assessed in terms of interfacial chemistry and microstructure. The mean interfacial fracture toughness, Gc, was found to decrease from 39...

متن کامل

Hydraulically pumped cone fracture in bilayers with brittle coatings

An earlier finite element modeling analysis of inner cone cracks in monolithic brittle solids subject to cyclic indentation in liquids is extended to include the case of a brittle layer bonded to a compliant substrate, using a model glass/polycarbonate bilayer system as an illustrative case study. Provision is made for incorporation of plate flexure stresses, along with hydraulic pumping stress...

متن کامل

Toughening Mechanisms in Nanolayered MAX Phase Ceramics—A Review

Advanced engineering and functional ceramics are sensitive to damage cracks, which delay the wide applications of these materials in various fields. Ceramic composites with enhanced fracture toughness may trigger a paradigm for design and application of the brittle components. This paper reviews the toughening mechanisms for the nanolayered MAX phase ceramics. The main toughening mechanisms for...

متن کامل

Possible phase transformation toughening of thermoset polymers by poly(butylene terephthalate)

Mechanisms were explored by which particles of poly(butylene terephthalate) (PBT) are able to toughen a brittle epoxy. The epoxy studied was an aromati(z amine-cured diglycidyl ether of bisphenoI-A, which was toughened at about twice the rate with particles of poly(butylene terephthalate) as with particles of nylon 6, poly(vinylidene fluoride), or CTBN rubber. Many of the mechanisms of tougheni...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Physical review letters

دوره 115 18  شماره 

صفحات  -

تاریخ انتشار 2015