Templated growth of diamond optical resonators via plasma-enhanced chemical vapor deposition

نویسندگان

  • X. Zhang
  • E. L. Hu
  • John A. Paulson
چکیده

We utilize plasma-enhanced chemical vapor deposition through a patterned silica mask for templated diamond growth to create optical resonators. The pyramid-shaped structures have quality factors Q up to 600, measured using confocal photoluminescence spectroscopy, and mode volumes V as small as 2:5ðk=nÞ for resonances at wavelengths k between 550 and 650 nm, and refractive index n, obtained using finite-difference time-domain simulations. Bright luminescence from nitrogen-vacancy and silicon-vacancy centers in the grown diamond is observed. The resonator design and fabrication technique obviates any etching of diamond, which preserves emitter properties in a pristine host lattice. Published by AIP Publishing. [http://dx.doi.org/10.1063/1.4961536]

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Determination of Optical Properties in Germanium Carbon Coatings Deposited by Plasma Enhanced Chemical Vapor Deposition

In this research, Germanium-carbon coatings were deposited on ZnS substrates by plasma enhanced chemical vapor deposition (PECVD) using GeH4 and CH4 precursors. Optical parameters of the Ge1-xCx coating such as refractive index, Absorption coefficient, extinction coefficient and band gap were measured by the Swanepoel method based on the transmittance spectrum. The results showed that the refra...

متن کامل

Evaluation of Vapor Deposition Techniques for Membrane Pore Size Modification

The suitability of three vapor deposition techniques for pore size modification was evaluated using polycarbonate track etched membranes as model supports. A feature scale model was employed to predict the pore geometry after modification and the resulting pure water flux. Physical vapor deposition (PVD) and pulsed plasma-enhanced chemical vapor deposition (PECVD), naturally, form asymmetric na...

متن کامل

Fabrication of Low Dislocation Density, Single-Crystalline Diamond via Two-Step Epitaxial Lateral Overgrowth

Continuous diamond films with low dislocation density were obtained by two-step epitaxial lateral overgrowth (ELO). Grooves were fabricated by inductively coupled plasma etching. Mo/Pd stripes sputtered in the grooves were used to inhibit the propagation of dislocations originating from the diamond substrate. Coalescent diamond films were achieved by ELO via microwave plasma-enhanced chemical v...

متن کامل

Optical properties of amorphous C/diamond thin films

Amorphous C/diamond films have been prepared by rf plasma enhanced vapor deposition from a CHdAr gas mixture. Infrared and optical-ultraviolet absorption characteristics are reported and used to characterize the bonding and optical properties of these films. It has been found that the optical band gap is not related to the hydrogen content in the films and varies according to the dc self bias d...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2016