STATEMENT OF THE PROBLEM Acidic foods and drinks can erode composite resins. Silorane-based composite is a new low shrinkage composite with higher hydrophobicity which might resist the erosive effect of beverages. PURPOSE The aim of this study was to determine the effects of 100% orange juice and non-alcoholic carbonated beer on microhardness of a silorane-based composite in comparison with two methacrylate-based composite resins. MATERIALS AND METHOD Ninety disc-shaped composite specimens were fabricated of Filtek P90, Filtek Z350 XT Enamel and Filtek Z250 (3M-ESPE) (n=30) and randomly divided into 3 subgroups of 10.Group 1 was immersed in distilled water, group 2 in 100% orange juice, and group 3 in non-alcoholic beer for 3 h/day. Primary, secondary and final Vickers microhardness tests were performed at the beginning of the study and 7 and 28 days later. Surface of 2 specimens in each group was evaluated under scanning electron microscope on day 28. Data were analyzed using repeated measures of ANOVA model (α=0.05). RESULTS The primary and secondary microhardness of P90 was significantly lower than that of Z350, and Z250 (p< 0.001). Microhardness of Z350 was also lower than that of Z250 (p= 0.002). On day 28, microhardness of P90 was lower than Z250 and Z350 (p< 0.001); however, microhardness values of Z250 and Z350 were not significantly different (p= 0.054). Microhardness of specimens subjected to non-alcoholic beer was significantly lower than that of controls (p= 0.003). Meanwhile, the microhardness value of resins in orange juice was somewhere between the two mentioned values with no significant difference with any of them (p> 0.05). CONCLUSION Although 28 days of immersion in 100% orange juice and non-alcoholic beer decreased the microhardness of all specimens, P90 experienced the greatest reduction of microhardness and non-alcoholic beer had the highest effect on reducing microhardness.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of energy drinks on microhardness of silorane and dimethacrylate-based composite resins

Introduction: Increased consumption of energy drinks has raised concerns about their effects on dental restorations. This study assessed the effects of two energy drinks on the surface microhardness of methacrylate and silorane-based composites after 1-week and 1-month periods. Materials & Methods: In this in-vitro study, 90 cubic samples were prepared from Filtek P90, Filtek Z250 and Filtek Z...

متن کامل

Effect of different bleaching strategies on microhardness of a silorane-based composite resin

Background. Dentists' awareness of the effects of bleaching agents on the surface and mechanical properties of restorative materials is of utmost importance. Therefore, this in vitro study was undertaken to investigate the effects of different bleaching strategies on the microhardness of a silorane-based composite resin. Methods. Eighty samples of a silorane-based composite resin (measuring 4 m...

متن کامل

Effect of a novel commercial potassium-oxalate containing tooth-desensitizing mouthrinse on the microhardness of resin composite restorative materials with different monomer compositions

BACKGROUND The effects of mouthrinses on dental resin composites have been investigated extensively. However, there is little information available regarding the effects of 'newly developed mouthrinse' formulations on the microhardness of different monomer based composite systems. Therefore, the aim of this study was to investigate the effect of a novel potassium-oxalate containing desensitizin...

متن کامل

The effect of bleaching on microhardness of silorane-based composite resins

Introduction: Bleaching treatments may negatively affect the surface quality of composite restorations existing in the mouth. This study sought to assess the effect of 16% and 35% carbamide peroxide on microhardness of silorane-based versus two methacrylate-based composite resins. Methods: A total of 54 discs were fabricated from FiltekP90 (P90), FiltekZ350XT(Z350) Enamel and Filtek Z250(Z25...

متن کامل

Comparison of Shear Bond Strength of Silorane and Methacrylate-Based Composites to IPS Empress 2 Ceramic with Various Surface Treatments

Objectives: Treatment of chipped or fractured porcelain with composite resin is considered as an economic treatment for minor fractures in ceramics. The aim of this study was to evaluate the effect of different ceramic surface treatments on bond strength of methacrylate-based and silorane-based composite resin to IPS Empress 2. Methods: Sixty IPS Empress 2 ceramic discs were fabrica...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 16  شماره 

صفحات  -

تاریخ انتشار 2015