Degradation of high-molecular-weight hyaluronan by hydrogen peroxide in the presence of cupric ions.

نویسندگان

  • Ladislav Soltés
  • Vlasta Brezová
  • Monika Stankovská
  • Grigorij Kogan
  • Peter Gemeiner
چکیده

Dynamic viscosity (eta) of the high-molecular-weight hyaluronan (HA) solution was measured by a Brookfield rotational viscometer equipped with a Teflon cup and spindle of coaxial cylindrical geometry. The decrease of eta of the HA solution, indicating degradation of the biopolymer, was induced by a system containing H2O2 alone or H2O2 plus CuCl2. The reaction system H2O2 plus CuCl2 as investigated by EPR spin-trapping technique revealed the formation of a four-line EPR signal characteristic of a *DMPO-OH spin adduct. Thus, hydroxyl radicals are implicated in degradation of high-molecular-weight HA by the system containing H2O2 and CuCl2.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Degradation of high-molar-mass hyaluronan and characterization of fragments.

A sample of high-molar mass hyaluronan was oxidized by seven oxidative systems involving hydrogen peroxide, cupric chloride, ascorbic acid, and sodium hypochlorite in different concentrations and combinations. The process of the oxidative degradation of hyaluronan was monitored by rotational viscometry, while the fragments produced were investigated by size-exclusion chromatography, matrix-assi...

متن کامل

Degradation of Transferrin in the Presence of Ascorbic Acid and Oxygen

The liberation of ammonia in the reaction of transferrin and ascorbic acid in phosphate buffer at pH 7.4, 37°C was investigated. It was found that transferrin is degraded in the reaction into smaller molecular weight polypeptides. The ammonia evolution was inhibited by catalase and by hydroxyl free radical trapping agents such as benzene, benzoate, and iodide. Dehydroascorbic acid and hydrogen ...

متن کامل

Protective effects of manganese(II) chloride on hyaluronan degradation by oxidative system ascorbate plus cupric chloride

The degradation of several high-molar-mass hyaluronan samples was investigated in the presence of ascorbic acid itself and further by an oxidative system composed of ascorbic acid plus transition metal ions, i.e. Fe(II) or Cu(II) ions. The latter oxidative system imitates conditions in a joint synovial fluid during early phase of acute joint inflammation and can be used as a model for monitorin...

متن کامل

Degradation of high-molar-mass hyaluronan by an oxidative system comprising ascorbate, Cu(II), and hydrogen peroxide: inhibitory action of antiinflammatory drugs--naproxen and acetylsalicylic acid.

Changes in dynamic viscosity of the solutions of a high-molar-mass hyaluronan (HA) were monitored using a rotational viscometer. The degradative conditions generated in the HA solutions by a system comprising ascorbate plus Cu(II) plus H(2)O(2) were studied either in the presence or absence of a drug--naproxen or acetylsalicylic acid. Continual decrease of the dynamic viscosity of HA solution w...

متن کامل

Journals on the Web

The antioxidative and/or free-radical-scavenging activities of R-()and S-(+)ibuprofen enantiomers, as well as of the drug racemate, were studied in vitro on measuring the kinetics of (uninhibited or drug-inhibited) degradation of high molecular weight hyaluronan by hydroxyl radicals. The continual flux of OH radicals radicals at aerobic conditions was maintained by the H2O2 + Cu 2+ system. The ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

عنوان ژورنال:
  • Carbohydrate research

دوره 341 5  شماره 

صفحات  -

تاریخ انتشار 2006