Theory for Hydrogen Desorption in Ferritic Steel

نویسندگان

  • Eun Ju Song
  • Dong-Woo Suh
  • H. K. D. H. Bhadeshia
چکیده

After a concise review of the analytical models available for the interpretation of thermal desorption rates for hydrogen effusion from steel, a numerical method that incorporates the essence of local equilibrium and detrapping kinetics has been implemented to account for the real complexity of practical experiments. For example, the model permits the treatment of multiple kinds of traps, uses very few fitting parameters, and has been tested against new experimental data and to assess the influence of a variety of variables such as trap density, on the nature of the desorption process. There remain, however, significant discrepancies when attempts are made to rationalise diverse observations reported in the literature. In particular, comparisons made between the trapping of hydrogen in pure iron and interstitial-free steel indicate a much stronger binding energy for hydrogen in the former case.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Deuterium retention and desorption behavior of reduced activated ferritic steel with surface damage due to high energy helium ion irradiation

Reduced activation ferritic-martensitic steel F82H was irradiated with 5 keV helium ions to introduce the surface damage. After the irradiation, the irradiated F82H was continuously exposed to 1.7 keV deuterium ions. The effects of the damages introduced by the helium ion irradiation on deuterium retention and desorption behavior of F82H were investigated. The HD desorption had a peak at around...

متن کامل

Hydrogen Embrittlement of Duplex Steel Tested Using Slow Strain Rate Test

P. Vaňová, J. Sojka. VŠB Technical u niversity of O strava, FMME, Ostrava, Czech Republic This paper is dealing with hydrogen embrittlement of austenitic-ferritic 2205 duplex steel using the slow strain rate test (SSRT). The original material was subjec ted to heat treatment under 700 °C during 5 hours and f ollowing aircooling with the aim of pr ovoking sigma phase pr ecipitation and embrittle...

متن کامل

Retention and release behaviors of plasma-loaded hydrogen in ferritic steels

In order to understand retention and release behaviors of plasma-loaded hydrogen in ferritic steels, hydrogen depth profiles were examined by means of a tritium imaging plate technique (TIPT). Hydrogen release was strongly affected by trapping effect in bulk and/or barrier effect of surface oxide layers during long term storage in air at room temperature (RT) and even heating in vacuum. Helium ...

متن کامل

Hydrogen-Induced Delayed Cracking in TRIP-Aided Lean-Alloyed Ferritic-Austenitic Stainless Steels

Susceptibility of three lean-alloyed ferritic-austenitic stainless steels to hydrogen-induced delayed cracking was examined, concentrating on internal hydrogen contained in the materials after production operations. The aim was to study the role of strain-induced austenite to martensite transformation in the delayed cracking susceptibility. According to the conducted deep drawing tests and cons...

متن کامل

Copper Manganese Spinel Coating on a Ferritic Stainless Steel for SOFC Application

Nowadays, Because of daily reduction of fossil fuels and environmental problems caused by using them, Fuel Cells attracted a major attention as clean and efficient way of generating electrical power. Solid Oxide Fuel Cells (SOFCs) have many advantages to other fuel cell types. High working temperature of SOFCs caused serious challenges including high oxidation rate of interconnects, Spallation ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2013