Laser-driven formation of a high-pressure phase in amorphous silica.

نویسندگان

  • Alberto Salleo
  • Seth T Taylor
  • Michael C Martin
  • Wendy R Panero
  • Raymond Jeanloz
  • Timothy Sands
  • François Y Génin
چکیده

Because of its simple composition, vast availability in pure form and ease of processing, vitreous silica is often used as a model to study the physics of amorphous solids. Research in amorphous silica is also motivated by its ubiquity in modern technology, a prominent example being as bulk material in transmissive and diffractive optics for high-power laser applications such as inertial confinement fusion (ICF). In these applications, stability under high-fluence laser irradiation is a key requirement, with optical breakdown occurring when the fluence of the beam is higher than the laser-induced damage threshold (LIDT) of the material. The optical strength of polished fused silica transmissive optics is limited by their surface LIDT. Surface optical breakdown is accompanied by densification, formation of point defects, cratering, material ejection, melting and cracking. Through a combination of electron diffraction and infrared reflectance measurements we show here that synthetic vitreous silica transforms partially into a defective form of the high-pressure stishovite phase under high-intensity (GW cm(-2)) laser irradiation. This phase transformation offers one suitable mechanism by which laser-induced damage grows catastrophically once initiated, thereby dramatically shortening the service lifetime of optics used for high-power photonics.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

بررسی تغییرات فازی سیلیس و سیلیسیوم به هنگام آسیاب کاری

In the present study phase transformation of silicon and silica during milling in different atmospheres was investigated. The silicon powder was subjected to high energy ball milling in ammonia (25%) atmosphere. The milled powder was subsequently annealed at 1200 ◦C for 1 hour. In another test a mixture of AlN and amorphous silica (micro silica) was subjected to high energy ball milling. The m...

متن کامل

Effect of Amorphous Silica Addition on Martensitic Phase Transformation of Zirconia and Investigation of its Tetragonal Structure Stability Mechanisms

This work is focused on the effect of amorphous SiO2 addition on the phase transformation and microstructural evolution of ZrO2 particles. Considering the structural similarities between the amorphous ZrO2 and its tetragonal structure, XRD results showed initial nucleation of metastable tetragonal ZrO2 from its amorphous matrix upon heat treatment. This metastable phase is unstable in pure ZrO2...

متن کامل

Synthesis of Si/MgO/Mg2SiO4 Composite from Rice Husk-Originated Nano-Silica

Silica exists in Rice husk, an agriculture waste, as a naturally occurring phase. In first step, acidic pre-treatment and calcination of the rice husk were performed to obtain nano-silica, in which various sizes of the nano-silica, totally with sizes under 80 nm, were achieved. Second, to reduce nano-silica to elemental Si and subsequently formation of the composite, Mg used as the reducing age...

متن کامل

Thermodynamics and kinetics of silica scaling

Silica scaling is probably the principal factor limiting the extraction of energy from high temperature geothermal systems. Silica exists in a number of polymorphs from quartz through to opal A (or amorphous silica). The thermodynamics of the solubility of quartz and amorphous silica with variations in temperature, salt content, pH and pressure are discussed. However, in silica saturated geothe...

متن کامل

A Comparison between the Effect of Cr and W Addition on Formation Kinetic of Nanostructure TiAl(γ) Alloy by Mechanical Alloying Route

In this research, mechanical alloying was used to produce Ti-50Al, Ti-45Al-5Cr and Ti-45Al-5W (at%) alloys. The effect of ternary addition (Cr and W) on microstructure and production efficiency of TiAl alloy were investigated. Alloying was performed in a planetary mill and the milling time varying from 5 to 70h. The structural evaluation in these powders was done by X-ray diffraction (XRD) tech...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Nature materials

دوره 2 12  شماره 

صفحات  -

تاریخ انتشار 2003