Shear testing of the porcelain-metal bond.

نویسندگان

  • J L Drummond
  • R G Randolph
  • V J Jekkals
  • J W Lenke
چکیده

A simple shear test was employed to determine the bonding strength of porcelain to a gold metal substrate and to a non-precious metal substrate after they had been aged in double-distilled water at 37 degrees C for four and 12 months. A 7.4% and 18.1% decrease in bond strength after four months and 12 months, respectively, was observed for the porcelain-gold system, and a decrease of 21.2% and 21.4% after four and 12 months, respectively, for the non-precious-porcelain system. A significant difference was observed between the bond strengths of the porcelain-metal composites: 51.17 +/- 11.29 MPa for the porcelain-gold system and 31.83 +/- 3.65 MPa for the porcelain-non-precious system.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Comparison of the Effect of Three methods of Porcelain Surface Treatment on Shear Bond Strength of Composite to Porcelain

Background and Aim: Several methods are available for intraoral repair of chipped porcelain restorations by composite resin. Also, there is still controversy regarding the best method of porcelain repair in terms of bond strength and cost effectiveness. This study aimed to compare three methods of porcelain surface treatment on shear bond strength (SBS) of composite to porcelain. Materials a...

متن کامل

A Comparative Evaluation of Shear Bond Strength of Creation Ceramic Veneer to Metal and Zirconia Cores

Abstract Background and Aim: High chipping rates of the veneering porcelain of zirconia ceramic restorations have been reported in clinical studies. Thus, the shear bond strength (SBS) between the zirconia core and veneering porcelain requires investigation. Materials and Methods: In this in-vitro study, at first, using a computer-aided design/computer-aided manufacturing (CAD/CAM) machine, 1...

متن کامل

Comparison of the Effect of Nd:YAG Laser and Sandblasting on Shear Bond Strength of a Commercial Ni-Cr Alloy to Porcelain

Introduction: Failures might occur at metal‒porcelain interfaces as a problem with metal‒ceramic restorations even with the application of airborne-particle abrasion technique. This study was undertaken to evaluate the effect of Nd:YAG laser treatment on the bond strength of porcelain fused to metal. Methods:  Twenty-four cylindrical specimens (4 mm in diameter and 4 mm in height) were made of ...

متن کامل

Effect of Opaque Porcelain Thickness Bond Strength of Porcelain to Ni-Cr Alloys

Objectives: Metal-ceramic restorations are the standard by which all esthetic restorations are measured. Fracture of dental restorations is a multifactorial problem, which is serious and costly. Debonding of porcelain from metal substructure and the bond strength depend on many factors. The purpose of this study was to determine whether or not the opaque porcelain thickness has a significant ef...

متن کامل

Shear bond strength between metal alloy and a ceramic system, submitted to different thermocycling immersion times.

The aim of this study was to evaluate the shear bond strength of Co-Cr and Ni-Cr metal alloys and a specific ceramic, submitted to different thermocycling immersion times. Sixty metal-ceramic specimens were confectioned and standardized in cylindricalformat. Three thermocycling conditions were evaluated: without thermocycling, 3,000 cycles (5 degrees C/55 degrees C+/-1) with 30s of immersion ti...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of dental research

دوره 63 12  شماره 

صفحات  -

تاریخ انتشار 1984