Hygrothermal Aging of Polyimide Matrix Composite Laminates

نویسنده

  • John A. Nairn
چکیده

Two polyimide-matrix systems were subjected to a series of hygrothermal aging experiments at various temperatures and relative humidities. For each aging condition, we measured the microcracking fracture toughness as a function of aging time. The toughness decreased with time. The rate of decrease increased with temperature and relative humidity. All experimental results could be fit to a simple first-order kinetics analysis where the degradation rate was assumed to be proportional to the total exposure to water above a threshold level below which no degradation occurs. The kinetics analysis was used to construct a hygrothermal aging master plot that can be used to make predictions of toughness degradation due to arbitrary hygrothermal environments. The master plot can be constructed from a few experiments on specimens immersed in water and thus is a potential accelerated test method for characterizing hygrothermal stability.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Environmental Effects on Mechanical Properties of Glass/Epoxy and Fiber Metal Laminates, Part I: Hygrothermal Aging

In this article, the effect of hygrothermal aging on mechanical properties of fiber metal laminates (FMLs) and E-glass/epoxy (GE) composites is investigated. First, FML and GE specimens were built using wet lay-up technique under vacuum pressure. Hygrothermal aging simulation was then carried out on both specimen types in distilled water at a constant temperature of 90 °C for 5 weeks. The resul...

متن کامل

The Effect of Hygrothermal Aging on the Microcracking Properties of of Some Carbon Fiber/Polyimide Laminates

When dry, quasi-isotropic, Avimid R © K polymer laminates were immersed in water at temperatures ranging from 35◦C to 95◦C, the water uptake initially had Fickian behavior, but later, after apparently reaching an equilibrium level of water saturation, showed a non-Fickian jump in uptake rate. Microscopy results showed that the secondary uptake process was caused by spontaneous formation of matr...

متن کامل

Flexural and Impact Properties of Stainless Steel based Glass Fibre Reinforced Fibre Metal Laminate under Hygrothermal Conditioning

Fibre metal laminates (FMLs) have appeared as the most suitable materials for shipbuilding, aeronautical and aerospace applications due to their superior mechanical properties over traditional materials. In this paper, degradation in flexural and impact properties of glass fibre/epoxy composite (GF/E composite) and stainless steel glass fibre/epoxy fibre metal laminate (SS FML) due to hygrother...

متن کامل

Multi-scale modelling of moisture diffusion coupled with stress distribution in CFRP laminated composites

Laminated composite structures operating in a marine environment are subject to moisture ingress. Due to the slow diffusion process of moisture, the distribution of moisture is not uniform so that the laminates can develop hygrothermal stresses. An accurate prediction of the moisture concentration and the associated hygrothermal stress is vital to the understanding of the effect of marine envir...

متن کامل

Moisture Diffusion Properties of Fabric Composite (Glass Fiber/Epoxy Resin)

In this study, the effect of hygrothermal conditioning on the moisture diffusion properties of the fabric composite (glass fiber/epoxy resin) was investigated. The water uptake of the specimens conditioned in humid environment at different relative humidities (0, 60 and 96 % r.h) at constant temperature (60°C) was evaluated by weight gain measurements. The moisture diffusion properties of the f...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 1999