Porous poly(L-lactic acid)/apatite composites created by biomimetic process.

نویسندگان

  • R Zhang
  • P X Ma
چکیده

Highly porous poly(L-lactic acid)/apatite composites were prepared through in situ formation of carbonated apatite onto poly(L-lactic acid) foams in a simulated body fluid. The highly porous polymer foams (up to 95% porosity) were prepared from polymer solution by solid-liquid phase separation and subsequent sublimation of the solvent. The foams were then immersed in the simulated body fluid at 37 degrees C to allow the in situ apatite formation. After incubation in the simulated body fluid for a certain period of time, a large number of characteristic microparticles formed on the surfaces of pore walls throughout the polymer foams. The microparticles were characterized with scanning electron microscopy, energy dispersive spectroscopy, Fourier transform IR spectroscopy, and X-ray diffractometry. These porous spherical microparticles were assemblies of microflakes. They were found to be carbonated bonelike apatite. A series of composite foams with varying sizes and concentrations of the apatite particles was obtained by varying incubation time and conditions. These porous composites may be promising scaffolding materials for bone tissue engineering and regeneration because the excellent bone-bonding properties of the apatite may provide a good environment for osteoblast and osteoprogenitor cells' attachment and growth.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Composite coating of bonelike apatite particles and collagen fibers on poly L-lactic acid formed through an accelerated biomimetic coprecipitation process.

Collagen and apatite were coprecipitated as a composite coating on poly L-lactic acid (PLLA) in an accelerated biomimetic process. The incubation solution contained collagen (1 g/L) and simulated body fluid with 5 times inorganic ionic concentrations as human blood plasma. The coating formed on PLLA films and scaffolds after a 24-h incubation was characterized by using energy-dispersive X-ray s...

متن کامل

PLLA scaffolds with biomimetic apatite coating and biomimetic apatite/collagen composite coating to enhance osteoblast-like cells attachment and activity

Novel scaffolds composed of poly(L-lactic acid) (PLLA) skeleton covered with bonelike apatite or apatite/collagen composite were produced via a combined phase-separation technique and an accelerated biomimetic coating process. Saos-2 osteoblast-like cells were used to evaluate the cellular behaviors on these biomimetic coatings. Cell morphologies on the surfaces of PLLA scaffolds, PLLA scaffold...

متن کامل

A Study of Bone-Like Apatite Formation on β-TCP/PLLA Scaffold in Static and Dynamic Simulated Body Fluid

The ability of apatite to form on the surface of biomaterials in simulated body fluid (SBF) has been widely used to predict the bone-bonding ability of bioceramic and bioceramic/polymer composites in vivo. Porous β-tricalcium phosphate/poly(L-lactic acid) (β-TCP/PLLA) composite scaffold was synthesized by new method. The ability of inducing calcium phosphate (Ca-P) formation was compared in sta...

متن کامل

Biomimetic mineralized strontium-doped hydroxyapatite on porous poly(l-lactic acid) scaffolds for bone defect repair

Introduction poly(l-lactic acid) (PLLA) has been approved for clinical use by the US Food and Drug Administration (FDA); however, their stronger hydrophobicity and relatively fast degradation rate restricted their widespread application. In consideration of the composition of bone, the inorganic-organic composite has a great application prospect in bone tissue engineering. Many inorganic-organi...

متن کامل

Heterotopic bone formation by nano-apatite containing poly(D,L-lactide) composites.

To render polymeric materials osteoinductive, nano-sized calcium phosphate apatite particles (CaP) were introduced into a low molecular weight poly(D,L-lactide). Homogenous composites were made with 10%, 20% and 40% by weight of apatite content while pure polylactide was used as control. Thereafter porous samples (pore size 300-400 microm, 60% porosity) were fabricated and sterilized. In vitro ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of biomedical materials research

دوره 45 4  شماره 

صفحات  -

تاریخ انتشار 1999