Application of X-ray Microtomography to Quantify the Liquid Fraction of M2 Steel for Semi-solid Forming process

نویسندگان

  • Guochao Gu
  • Raphaël Pesci
  • Eric Becker
  • Laurent Langlois
  • Régis Bigot
  • Guochao GU
  • Raphaël PESCI
  • Eric BECKER
  • Laurent LANGLOIS
  • Régis BIGOT
چکیده

Thixoforging, one variant of semi-solid metal processing in which the metallic alloys are processed at low liquid fraction (0.1< Fl < 0.3), is used to produce complex parts with high mechanical properties. Steel thixoforging faces more challenges as compared to that of low melting point materials due to high processing temperature and lack of understanding of the thermomechanical behavior of materials in the given conditions. It is crucial to study the microstructure in the semi-solid state to improve the understanding of the thixoforging process since the material behavior strongly depends on main parameters: the liquid fraction, its distribution as well as the coherence of the solid skeleton. The microstructure has a great influence on the viscosity of the material, on the flows and finally on the final shape and mechanical properties of the thixoforged parts. Here, the characterization of the volume fraction and distribution of liquid in the semi-solid state with high energy 3D X-ray microtomography is investigated on M2 steel grade as a ‘model’ alloy. The obtained results are compared to 2D observations using EDS technique in SEM on heated and quenched specimens. They show a good correlation making both approaches very efficient for the study of the liquid zones in the semi-solid state.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Determination of quantity and localization of liquid in the semi-solid state using both 3D X-ray microtomography and 2D techniques for steel thixoforming

The distribution of liquid at the semi solid state is one of the most important parameters for steel thixoforging. It has a great influence on the viscosity of the material, on the flows and finally on the final shape and mechanical properties of the thixoforged parts. Both ex situ and in situ 3D X-ray microtomography characterizations have been carried out to determine the quantity and localiz...

متن کامل

In Situ Microstructure Observation Of Steel Grades In The Semi-Solid State For Thixoforging Process By Using Confoncal Laser Scanning Microscopy

The microstructure plays a crucial role for steel semi-solid forming process, and particularly for the steel thixoforging process, since it determines the thixotropic flow behavior of materials in the semi-solid state. Therefore, it is necessary to well understand the microstructure evolution during high speed heating and forming. Classically, it is investigated on a solid material quenched fro...

متن کامل

Microstructural Evolution during DPRM Process of Semisolid Ledeburitic D2 Tool Steel

Semisolid metal processing is a relatively new technology that offers several advantages over liquid processing and solid processing because of the unique behaviour and characteristic microstructure of metals in this state. With the aim of finding a minimum process chain for the manufacture of high-quality production at minimal cost for forming, the microstructural evolution of the ledeburitic ...

متن کامل

Effect of Temperature and Time on the Joint Properties of AISI420 Steel to SAF2507 Steel Produced by Transient Liquid Phase Process

In this research, the effect of temperature and time on the properties of AISI420/SAF2507 dissimilar joint produced by transient liquid phase bonding process was investigated. A BNi-2 interlayer with 25 μm thickness was inserted between two dissimilar steel samples. The bonding process was performed at 1050 oC and 1100 oC for different bonding times. The microstructures of the joints were studi...

متن کامل

An Investigation on Mechanical Properties of Ultrafine Grained 316 Stainless Steel by Thermomechanical Treatment

In this paper, an advanced thermo-mechanical treatment was conducted on AISI 316 austenitic stainless steel. At first, three samples were rolled at the ambient temperature, the temperature of -20 ºC (dry ice and ethanol) and -196 ºC (liquid nitrogen). Then, the samples were annealed at 800 ºC in the time range of 1 to 15 minutes. In each step, the microhardness values of the samples were measur...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2017