Improved Formula for the Stress Intensity Factor of Semi-Elliptical Surface Cracks in Welded Joints under Bending Stress

نویسندگان

  • Yang Peng
  • Chao Wu
  • Yifu Zheng
  • Jun Dong
چکیده

Welded joints are prone to fatigue cracking with the existence of welding defects and bending stress. Fracture mechanics is a useful approach in which the fatigue life of the welded joint can be predicted. The key challenge of such predictions using fracture mechanics is how to accurately calculate the stress intensity factor (SIF). An empirical formula for calculating the SIF of welded joints under bending stress was developed by Baik, Yamada and Ishikawa based on the hybrid method. However, when calculating the SIF of a semi-elliptical crack, this study found that the accuracy of the Baik-Yamada formula was poor when comparing the benchmark results, experimental data and numerical results. The reasons for the reduced accuracy of the Baik-Yamada formula were identified and discussed in this paper. Furthermore, a new correction factor was developed and added to the Baik-Yamada formula by using theoretical analysis and numerical regression. Finally, the predictions using the modified Baik-Yamada formula were compared with the benchmark results, experimental data and numerical results. It was found that the accuracy of the modified Baik-Yamada formula was greatly improved. Therefore, it is proposed that this modified formula is used to conveniently and accurately calculate the SIF of semi-elliptical cracks in welded joints under bending stress.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Estimation of the Stress Intensity Factors for Surface Cracks in Spherical Electrode Particles Subject to Phase Separation

Experiments have frequently shown that phase separation in lithium-ion battery electrodes could lead to the formation of mechanical defects, hence causing capacity fading. The purpose of the present work has been to examine stress intensity factors for pre-existing surface cracks in spherical electrode particles during electrochemical deintercalation cycling using both analytical and numerical ...

متن کامل

Evaluating Weld Magnification Factor in Welded Tubular Joints Using Artifitial Neural Networks

In welded tubular joints, when the fatigue crack depth is less than 20% of chord wall thickness, the crack growing process is highly affected by weld geometry.&#10 Hence, T-butt solution and weld magnification factor (Mk) are applicable tools for evaluating the crack growth rate in this domain. In this research, the capability of Artificial Neural Network (ANN) for estimating the Mk of weld toe...

متن کامل

Evaluating Weld Magnification Factor in Welded Tubular Joints Using Artifitial Neural Networks

In welded tubular joints, when the fatigue crack depth is less than 20% of chord wall thickness, the crack growing process is highly affected by weld geometry. Hence, T-butt solution and weld magnification factor (Mk) are applicable tools for evaluating the crack growth rate in this domain. In this research, the capability of Artificial Neural Network (ANN) for estimating the Mk of weld toe c...

متن کامل

Developments in the Analysis of Interacting Cracks

-This paper presents an overview of the finite element alternating technique for the analysis of interacting cracks. To illustrate the ease and accuracy of this method the technique is used to analyse several problems associated with both widespread fatigue and multi-site damage, a problem which is attracting worldwide attention. Whilst this paper presents an overview of the technique for both ...

متن کامل

Stress Intensity Factor Expression for Welded Butt Joint with Undercut and Inclined Lack of Penetration Defects considering the Effect of Joint Shape

In this paper, the stress intensity factor (SIF) expression for defected butt welds containing undercut and inclined lack of penetration (LOP) subject to far-field tensile stress is derived. Some of the standards such as ISO 5817 and BS EN 25817 have specified allowable limits for the length of the undercut and LOP defects and for the height of the weld. In addition, EN 29692 standard has deter...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 10  شماره 

صفحات  -

تاریخ انتشار 2017