Impact of pore size on the vascularization and osseointegration of ceramic bone substitutes in vivo.

نویسندگان

  • Frank M Klenke
  • Yuelian Liu
  • Huipin Yuan
  • Ernst B Hunziker
  • Klaus A Siebenrock
  • Willy Hofstetter
چکیده

The repair of bone defects with biomaterials depends on a sufficient vascularization of the implantation site. We analyzed the effect of pore size on the vascularization and osseointegration of biphasic calcium phosphate particles, which were implanted into critical-sized cranial defects in Balb/c mice. Dense particles and particles with pore sizes in the ranges 40-70, 70-140, 140-210, and 210-280 microm were tested (n = 6 animals per group). Angiogenesis, vascularization, and leukocyte-endothelium interactions were monitored for 28 days by intravital microscopy. The formation of new bone and the bone-interface contact (BIC) were determined histomorphometrically. Twenty-eight days after implantation, the functional capillary density was significantly higher with ceramic particles whose pore sizes exceeded 140 microm [140-210 microm: 6.6 (+/-0.8) mm/mm(2); 210-280 microm: 7.3 (+/-0.6) mm/mm(2)] than with those whose pore sizes were lesser than 140 microm [40-70 microm: 5.3 (+/-0.4) mm/mm(2); 70-140 microm: 5.6 (+/-0.3) mm/mm(2)] or with dense particles [5.7 (+/-0.8) mm/mm(2)]. The volume of newly-formed bone deposited within the implants increased as the pore size increased [40-70 microm: 0.07 (+/-0.02) mm(3); 70-140 microm: 0.10 (+/-0.06) mm(3); 140-210 microm: 0.13 (+/-0.05) mm(3); 210-280 microm: 0.15 (+/-0.06) mm(3)]. Similar results were observed for the BIC. The data demonstrates pore size to be a critical parameter governing the dynamic processes of vascularization and osseointegration of bone substitutes.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Improving the mechanical and bioactivity of hydroxyapatite porous scaffold ceramic with diopside/forstrite ceramic coating

Objective(s): Scaffolds are considered as biological substitutes in bone defects which improve and accelerate the healing process of surrounding tissue. In recent years a major challenge in biomaterials is to produce porous materials with properties similar to bone tissue. In this study, the natural bioactive hydroxyapatite scaffolds with nano Diopside /Forstrite coating was successfully synthe...

متن کامل

Biological Properties of Solid Free Form Designed Ceramic Scaffolds with BMP-2: In Vitro and In Vivo Evaluation

Porous ceramic scaffolds are widely studied in the tissue engineering field due to their potential in medical applications as bone substitutes or as bone-filling materials. Solid free form (SFF) fabrication methods allow fabrication of ceramic scaffolds with fully controlled pore architecture, which opens new perspectives in bone tissue regeneration materials. However, little experimentation ha...

متن کامل

Bone Substitute Effect on Vascularization and Bone Remodeling after Application of phVEGF165 Transfected BMSC

VEGF (vascular endothelial growth factor) promotes vascularization and remodeling of bone substitutes. The aim of this study was to examine the effect of distinct resorbable ceramic carriers on bone forming capacities of VEGF transfected bone marrow stromal cells (BMSC). A critical size defect of the radius in rabbits was filled either by a low surface scaffold called beta-TCP (tricalciumphspha...

متن کامل

Porous ceramic bone scaffolds for vascularized bone tissue regeneration.

Hydroxyapatite scaffolds with a multi modal porosity designed for use in tissue engineering of vascularized bone graft substitutes were prepared by three dimensional printing. Depending on the ratio of coarse (mean particle size 50 microm) to fine powder (mean particle size 4 microm) in the powder granulate and the sintering temperature total porosity was varied from 30% to 64%. While macroscop...

متن کامل

Corrosion Properties of 70SiO2-15TiO2-15ZrO2 Ceramic Membrane

The 70SiO2-15TiO2-15ZrO2 membrane was prepared by a sol-gel procedure. The corrosion behavior of microporous toplayers along with the membrane characterization in terms of pore size, surface area, pore volume and weight loss is described. The final ceramic membrane with a thickness of 400 nm and uniform surface was obtained. This membrane confirmed the fine microporous characteristic with mean ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

عنوان ژورنال:
  • Journal of biomedical materials research. Part A

دوره 85 3  شماره 

صفحات  -

تاریخ انتشار 2008