Aging characteristics and mechanical properties of 1600 MPa body-centered cubic Cu and B2-NiAl precipitation-strengthened ferritic steel

نویسندگان

  • Monica Kapoor
  • Dieter Isheim
  • Gautam Ghosh
  • Semyon Vaynman
  • Morris E. Fine
چکیده

High-strength low-carbon ferritic steels attaining a maximum yield strength of 1600 MPa by combined Cu and NiAl precipitationstrengthening were developed. The yield strength of the alloys increases monotonically with the total concentration of the principal alloying elements i.e. Mn, Cu, Ni and Al. At 12.40 at.%, a 1600 MPa yield strength is achieved after solution treatment at 950 C followed by aging at 550 C for 2 h. For all three alloys investigated, the hardness reached a maximum after 1–2 h aging at 500–550 C. At peak hardness, the combined precipitation of the body-centered cubic (bcc) Cu-alloy and B2-ordered NiAl-type intermetallic precipitates is observed by atom probe tomography (APT). The morphology, composition and structure of the Cu-alloy and NiAl-type precipitates were characterized using APT and transmission electron microscopy, as a function of aging time at 550 C. In peak hardness conditions, the equiaxed bcc Cu-alloyed precipitates contain substantial amounts of Fe and are enriched in Ni, Al and Mn. Ni and Mn segregate at the Cu-alloy precipitate/ferrite matrix interface. In addition to the segregation, B2 NiAl-type precipitates nucleate at the Cu-alloy precipitates. After aging for 2 h, most Cu-alloy precipitates have a NiAl-type precipitate attached to their side. On subsequent further aging, the Cu-alloyed precipitates enrich progressively with Cu and elongate, indicating a transformation to the 9R or face centered cubic structure. The Cu-alloyed precipitates coarsen slower than the NiAl-type precipitates due to interfacial energy differences between the two types of precipitates, slower diffusion kinetics of Cu through the NiAl precipitates, different matrix equilibrium solubility and solute transfer from Cu-alloyed precipitates to NiAl-type precipitates. The relatively slow growth and coarsening of Cu-alloyed precipitates are consistent with the observation of an only modest decrease of hardness with extended aging. 2014 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of strain rate and temperature on mechanical properties and fracture mode of high strength precipitation hardened ferritic steels

The effect of strain rate on the flow stress of a low carbon high strength ferritic steel that contains nanometer size Cu–Ni–Al precipitates is found to be much less than that of HSLA 65 that does not have such precipitates. This result is in agreement with the theory that such precipitates locally lower the Peierls stress for screw dislocations in body-centered cubic iron. The fracture mode in...

متن کامل

Nano-sized precipitate stability and its controlling factors in a NiAl-strengthened ferritic alloy

Coherent B2-ordered NiAl-type precipitates have been used to reinforce solid-solution body-centered-cubic iron for high-temperature application in fossil-energy power plants. In this study, we investigate the stability of nano-sized precipitates in a NiAl-strengthened ferritic alloy at 700-950 °C using ultra-small angle X-ray scattering and electron microscopies. Here we show that the coarsenin...

متن کامل

Super-tough Steel for Bridges and Other Applications

Addition of titanium (Ti) to ASTM A710 Grade B Cu-precipitation-strengthened steel significantly increases the impact absorbed fracture energy and reduces the ductile-to-brittle transition temperature. The effect of Ti correlates with the reduction of the amount of pearlite in the ferritic microstructure. A thorough study of the mechanical properties of Ti-modified A 710-B steel is presented.

متن کامل

Load partitioning between the bcc-iron matrix and NiAl-type precipitates in a ferritic alloy on multiple length scales

An understanding of load sharing among constituent phases aids in designing mechanical properties of multiphase materials. Here we investigate load partitioning between the body-centered-cubic iron matrix and NiAl-type precipitates in a ferritic alloy during uniaxial tensile tests at 364 and 506 °C on multiple length scales by in situ neutron diffraction and crystal plasticity finite element mo...

متن کامل

Mechanical Behavior and Fracture Properties of NiAl Intermetallic Alloy with Different Copper Contents

The deformation behavior and fracture characteristics of NiAl intermetallic alloy containing 5~7 at% Cu are investigated at room temperature under strain rates ranging from 1 ˆ 10 ́3 to 5 ˆ 103 s ́1. It is shown that the copper contents and strain rate both have a significant effect on the mechanical behavior of the NiAl alloy. Specifically, the flow stress increases with an increasing copper con...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2014