Shear bond strength between veneering ceramics and ceria-stabilized zirconia/alumina.

نویسندگان

  • Jens Fischer
  • Bogna Stawarczyk
  • Irena Sailer
  • Christoph H F Hämmerle
چکیده

STATEMENT OF PROBLEM Ceria-stabilized tetragonal ZrO(2)/Al(2)O(3) nanocomposite (Ce-TZP/A) offers superior properties compared to yttria-stabilized zirconia (Y-TZP). However, the bond quality to veneering ceramics has not been investigated. PURPOSE The purpose of this study was to evaluate the bond strength of different veneering ceramics to Ce-TZP/A. MATERIAL AND METHODS Cubes of Ce-TZP/A (NANOZR) (edge length, 10 mm) were layered with veneering ceramics (5 mm in thickness) with or without application of a liner and sheared at the interface. The effect of different surface treatments (polished with 3-mum diamond paste or airborne-particle abraded) was evaluated with 1 veneering ceramic (Cerabien ZR). Shear bond strength of 5 additional veneering ceramics (IPS e.max, Initial ZR, Triceram, Vintage ZR, or VITA VM 9) to polished Ce-TZP/A was measured (n=10). Polished Y-TZP (Hint-ELs ZrO(2) HIP) veneered with 2 ceramics (Cerabien ZR, Vintage ZR) served as the control. Mean shear bond strength values (MPa) were calculated. The means were statistically analyzed with 2-way ANOVA for the effect of surface treatment and liner, 2-way ANOVA for the effect of different veneering ceramic brands and liner, and 3-way ANOVA for the effect of substrate, veneering ceramic brands, and liner, as well as 1-way ANOVA for the differences between the veneering ceramics. A post hoc Scheffé test was used (alpha=.05). RESULTS The effects of surface treatment (P=.007) or application of liner (P<.001) were significant. Shear bond strength with different veneering ceramics showed bond strength values with means ranging between 14.2 +/-1.7 MPa (IPS e.max with liner) and 27.5 +/-4.2 MPa (VITA VM 9). A significant difference was found between the results of shear bond tests with Y-TZP and Ce-TZP/A (P=.022). The application of a liner on Y-TZP had no significant effect. CONCLUSIONS Airborne-particle abrasion is not necessary to enhance the shear bond strength of the evaluated veneering ceramics to Ce-TZP/A. Liners impair the shear bond strength of veneering ceramics to Ce-TZP/A.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites.

Aim of the investigation was to assess the effect of different surface treatments on the bond strength of veneering ceramics to zirconia. In a shear test, the influences of polishing, sandblasting, and silica-coating of the zirconia surface on bonding were assessed with five different veneering ceramics. In addition the effect of liner application was examined. With one veneering ceramic, the i...

متن کامل

Effect of cooling rate on shear bond strength of veneering porcelain to a zirconia ceramic material.

The purpose of the present study was to evaluate the effect of cooling rates after firing procedures of veneering porcelain on shear bond strength between veneering porcelain and a zirconium dioxide (zirconia; ZrO₂) ceramic material. A total of 48 ZrO₂ disks were divided equally into three groups. Two veneering porcelains that are recommended for ZrO₂ material - Cerabien ZR (CZR), IPS e.max Cer...

متن کامل

Current status of zirconia restoration.

During the past decade, zirconia-based ceramics have been successfully introduced into the clinic to fabricate fixed dental prostheses (FDPs), along with a dental computer-aided/computer-aided manufacturing (CAD/CAM) system. In this article (1) development of dental ceramics, (2) the current status of dental CAD/CAM systems, (3) CAD/CAM and zirconia restoration, (4) bond between zirconia and ve...

متن کامل

Shear bond strength in zirconia veneered ceramics using two different surface treatments prior veneering.

Aim of the study was to assess the effect of different surface treatments on the shear bond strength (SBS) of the veneering ceramics to zirconia core. In a shear test the influence of grinding and sandblasting of the zirconia surface on bonding were assessed. Statistical analysis was performed using SPSS statistical package (version 17.0, SPSS Inc., Chicago, IL, USA) and Microsoft Office Excel ...

متن کامل

Shear bond strength of veneering ceramic to coping materials with different pre-surface treatments

PURPOSE Pre-surface treatments of coping materials have been recommended to enhance the bonding to the veneering ceramic. Little is known on the effect on shear bond strength, particularly with new coping material. The aim of this study was to investigate the shear bond strength of veneering ceramic to three coping materials: i) metal alloy (MA), ii) zirconia oxide (ZO), and iii) lithium disili...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • The Journal of prosthetic dentistry

دوره 103 5  شماره 

صفحات  -

تاریخ انتشار 2010