Effect of Antimony Additions on Corrosion and Mechanical Properties of Sn-Bi Eutectic Lead-Free Solder Alloy

نویسندگان

  • Alberto Torres
  • Luis Hernández
  • Octavio Domínguez
چکیده

The goal of the present work is to investigate the effects of the addition of Sb (0, 3 and 6 wt%) on structure, melting, corrosion and mechanical properties of Sn-Bi eutectic solder alloys. The mechanical properties of the bulk Sn-Bi-Sb solders were higher as the amount of antimony increases, making compressive strength augment from 65 MPa to 100 MPa when 6 wt% Sb was incorporated to the Sn-Bi eutectic alloy. The three alloys presented a melting temperature that is smaller to the one exhibited by the eutectic alloy Sn-38Pb (Tm = 183 ̊C). According to the electrochemical results, the addition of higher contents of Sb to the Sn-Bi eutectic alloy had a positive effect: it ennobled the Ecorr values.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effects of a Third Element on Microstructure and Mechanical Properties of Eutectic Sn–Bi Solder

The effects of a third element, namely silver, copper, zinc, or antimony, on the microstructure and mechanical properties of eutectic tin-bismuth (Sn–Bi) solder were investigated. The investigation showed that, except for zinc, the addition of a trace amount of the third element improves the ductility of the Sn–Bi solder owing to the formation of a fine, homogeneous ternary eutectic microstruct...

متن کامل

Investigation of microstructure and physical properties in nanocomposite solder reinforced with various percent of graphene nanosheets (SAC0307+GNSs)

Development of electronic industries, compression of electronic equipment, and removing lead from electronic circuits for environmental issues, resulted in a significant challenge in design and development of tin-based lead-free solders with physical and mechanical properties similar to old tin-lead alloys. In this regard, the set of Sn-Ag-Cu alloys with eutectic and near eutectic compositions ...

متن کامل

Investigation of microstructure and physical properties in nanocomposite solder reinforced with various percent of graphene nanosheets (SAC0307+GNSs)

Development of electronic industries, compression of electronic equipment, and removing lead from electronic circuits for environmental issues, resulted in a significant challenge in design and development of tin-based lead-free solders with physical and mechanical properties similar to old tin-lead alloys. In this regard, the set of Sn-Ag-Cu alloys with eutectic and near eutectic compositions ...

متن کامل

Mechanical Properties and Solder Joint Reliability of Low-Melting Sn-Bi-Cu Lead Free Solder Alloy

The influence of alloy composition of lowmelting Sn-Bi-Cu lead-free solder alloys on mechanical properties and solder joint reliabilities were investigated. The mechanically optimum alloy composition is Sn-40Bi-0.1Cu (mass%). The addition of 40mass%Bi improves the ductility and restrains the fillet-lifting, which are problems of lead-free solders with Bi. The addition of copper improves both th...

متن کامل

Novel Rare-Earth-Containing Lead-Free Solders with Enhanced Ductility

Several lead-free material systems are available as replacements for traditional lead-based solders in microelectronic packaging, including near-eutectic combinations of tin-rich alloys. Although these materials have superior mechanical properties as compared to the Pb-Sn system, much work remains in developing these materials for electronic packaging. Small additions of rare-earth elements hav...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2013