In order to design composites and laminated materials, it is necessary to understand the issues that govern crack deflection and crack penetration at interfaces. Historically, models of crack deflection have been developed using either a strength-based or an energy-based fracture criterion. However, in general, crack propagation depends on both strength and toughness. Therefore, in this paper, crack deflection has been studied using a cohesive-zone model which incorporates both strength and toughness parameters simultaneously. Under appropriate limiting conditions, this model reproduces earlier results that were based on either strength or energy considerations alone. However, the general model reveals a number of interesting results. Of particular note is the apparent absence of any lower bound for the ratio of the substrate to interface toughness to guarantee crack penetration. It appears that, no matter how tough an interface is, crack deflection can always be induced if the strength of the interface is low enough compared to the strength of the substrate. This may be of significance for biological applications where brittle organic matrices can be bonded by relatively tough organic layers. Conversely, it appears that there is a lower bound for the ratio of the substrate strength to interfacial strength, below which penetration is guaranteed no matter how brittle the interface. Finally, it is noted that the effect of modulus mismatch on crack deflection is very sensitive to the mixed-mode failure criterion for the interface, particularly if the cracked layer is much stiffer than the substrate. ∗Current address: Department of Mechanical Engineering, Oregon State University, Corvallis, OR 97331

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mixed-mode Cohesive-zone Models for Delamination and Deflection in Composites

Cohesive-zone models for interfaces incorporate both strength and energy parameters. Therefore, they provide a natural bridge between strength-based models and energy-based models for fracture, allowing delamination to be described by a single framework that covers a range of applications for which the strength or energy criteria alone might not be sufficient. In this paper, the relationships b...

متن کامل

On the toughening of brittle materials by grain bridging: promoting intergranular fracture through grain angle, strength, and toughness

The structural reliability of many brittle materials such as structural ceramics relies on the occurrence of intergranular, as opposed to transgranular, fracture in order to induce toughening by grain bridging. For a constant grain boundary strength and grain boundary toughness, the current work examines the role of grain strength, grain toughness, and grain angle in promoting intergranular fra...

متن کامل

The weak interfaces within tough natural composites: experiments on three types of nacre.

Mineralization is a typical strategy used in natural materials to achieve high stiffness and hardness for structural functions such as skeletal support, protection or predation. High mineral content generally leads to brittleness, yet natural materials such as bone, mollusk shells or glass sponge achieve relatively high toughness considering the weakness of their constituents through intricate ...

متن کامل

STRENGTH AND FRACTURE TOUGHNESS OF WHISKER REINFORCED DENTAL RESIN-BASED COMPOSITES

Enhancing the properties of dental resin composites is of interest to researchers. The objective of the present investigation was to improve the strength and fracture toughness of dental composites via addition of silicon carbide whiskers and substitution of commonly used filler materials with stabilized zirconia ceramic powder. It was also intended to study the effect of powder- to- whisker ra...

متن کامل

Cymbiola nobilis shell: Toughening mechanisms in a crossed-lamellar structure

Natural structural materials with intricate hierarchical architectures over several length scales exhibit excellent combinations of strength and toughness. Here we report the mechanical response of a crossed-lamellar structure in Cymbiola nobilis shell via stepwise compression tests, focusing on toughening mechanisms. At the lower loads microcracking is developed in the stacked direction, and c...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2005