Recovery of cobalt and lithium from spent lithium ion batteries using organic citric acid as leachant.

نویسندگان

  • Li Li
  • Jing Ge
  • Feng Wu
  • Renjie Chen
  • Shi Chen
  • Borong Wu
چکیده

In this work, a hydrometallurgical process based on leaching is applied to recover cobalt and lithium from spent lithium ion batteries (LIBs). Citric acid and hydrogen peroxide are introduced as leaching reagents and the leaching of cobalt and lithium with a solution containing C(6)H(8)O(7) x H(2)O is investigated. When both C(6)H(8)O(7) x H(2)O and H(2)O(2) are used an effective recovery of Li and Co as their respective citrates is possible. The leachate is characterized by scanning electron micrography (SEM) and X-ray diffraction (XRD). The proposed procedure includes the mechanical separation of metal-containing particles and a chemical leaching process. Conditions for achieving a recovery of more than 90% Co and nearly 100% Li are achieved experimentally by varying the concentrations of leachant, time and temperature of the reaction as well as the starting solid-to-liquid ratio. Leaching with 1.25 M citric acid, 1.0 vol.% hydrogen peroxide and a S:L of 20 g L(-1) with agitation at 300 rpm in a batch extractor results in a highly efficient recovery of the metals within 30 min of the processing time at 90 degrees C. This hydrometallurgical process is found to be simple, environmentally friendly and adequate for the recovery of valuable metals from spent LIBs.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Voltage increase of aqueous lithium-ion batteries by Li-ion conducting Li1.5Al0.5Ge1.5(PO4)3 glass-ceramic

  In this research, a lithium ion conducting lithium aluminum germanium phosphate (LAGP) glass-ceramic with a formula of Li1.5Al0.5Ge1.5(PO4)3 was synthesized by melt-quenching method and subsequent crystallization at 850 °C for 8 h. The prepared glass-ceramic was characterized using X-ray diffraction analysis (XRD) and field emission scanning electron microscopy (FESEM). The XRD patterns exhib...

متن کامل

Recovery of cobalt sulfate from spent lithium ion batteries by reductive leaching and solvent extraction with Cyanex-272

Cobalt sulfate was recovered from crushed and screened prismatic type spent lithium ion batteries (LIBs) containing 5~20 % Co, 5~7 % Li, 5~10 % Ni, 15% organic chemicals, and 7% plastics together with Cu, Al, Fe, and Mn. Cobalt was reductively leached from the -16 mesh fraction in 1 h by stirring with 2 M H2SO4 and 6 vol% H2O2, at 60 C and 300 rpm using a solid/liquid ratio of 100 g/L to give a...

متن کامل

فروشویی زیستی دومرحله‌ای فلزات لیتیم، کبالت و منگنز از باتری های مستعمل لیتیم-یون سکه ای با استفاده از باکتری اسیدی‌تیوباسیلوس فرواکسیدانس

Background and Objective: Batteries can be hazardous to the environment and human health due to their toxic compounds. In this study, for detoxification and recovery of metals from spent coin batteries, a two-step bioleaching using Acidithiobacillus ferrooxidans was investigated. Materials and Methods: A number of spent coin batteries were powdered. The powder was added to the bacterial cultur...

متن کامل

بهینه‌سازی فرایند انحلال انتخابی لیتیم از باتری لیتیم- یون مستعمل توسط اگزالیک اسید با به‌کارگیری روش رویه پاسخ

In this study, the recovery of lithium from the cathode of the spent Li-ion batteries of the LiNixMnyCozO2 type was investigated. After complete discharging and dismantling, the cathodic section was cut and its aluminum content was selectively dissolved in 2.5 M NaOH solution at room temperature for 2 hr. In the next step, selective dissolution of lithium by oxalic acid from the de-aluminized c...

متن کامل

Initial Discharge Capacity of Manganese Cobaltite as Anode Material for Lithium Ion Batteries

Nanostructured manganese cobalt oxide spinel (MnCo2O4) are prepared by co-precipitation method and calcined at 650 and 750°C. Morphological studies show that by increasing the calcination temperature from 650 to 750°C, morphology of the particles changes from quasi-plate to polyhedral. The MnCo2O4 calcined at 650°C could deliver an initial discharge capacity of 1438 mAh g-1 under current densit...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of hazardous materials

دوره 176 1-3  شماره 

صفحات  -

تاریخ انتشار 2010