PURPOSE The aim of this study was to evaluate the efficiency of manual polishing over autoglazed and overglazed porcelain and their effect on plaque accumulation. MATERIALS AND METHODS Thirty-six porcelain discs were fabricated out of which 18 each was subjected for autoglazing and overglazing. Half surface of the discs was left intact; the remaining half was roughened with medium grit diamond bur. Roughened surfaces were repolished by porcelain polishing kits (Shofu, DFS, Eve). All the surfaces were evaluated by the perthometer and SEM. Six discs from each sample were placed in human volunteer's mouth for 72 hours to evaluate the plaque accumulation. Acquired data was subjected to ANOVA comparative evaluation. RESULTS Roughened surfaces had average roughness value of 2.88±0.1935 µm. The repolished surfaces by porcelain correction kits Shofu, DFS and Eve, average roughness value reduced to 0.6250±0.1036, 0.9192±0.0953, 0.9017±0.1305 respectively. Autoglazed and overglazed surfaces showed the mean roughness value (Ra) of 0.4217±0.0685, 0.3450±0.0729. SEM study showed the improved surfaces when subjected for polishing. Plaque accumulation percentage was the highest on roughened surface (93.83±6.2552%), followed by porcelain discs polished by commercial kits. Autoglazed surfaces found to be the best surfaces with the least plaque accumulation (0.5237±0.4209%). CONCLUSION All the polishing kits used in the study reduced the average roughness by approximately 77%. Corrected porcelain surfaces should ideally be reglazed, alternatively, polish the surfaces before final cementation.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Evaluation of the effect of a home bleaching agent on surface characteristics of indirect esthetic restorative materials--part II microhardness.

BACKGROUND The exponential usage of esthetic restorative materials is beholden to society needs and desires. Interaction between the bleaching agents and the esthetic restorative materials is of critical importance. AIM This in vitro study has been conducted to evaluate the effect of a home bleaching agent, carbamide peroxide (CP) 38%, on the microhardness of the fiber reinforced composite (F...

متن کامل

An evaluation of wear of human enamel opposed by ceramics of different surface finishes

STATEMENT OF PROBLEM Surface of porcelain restoration is a matter of clinical concern because of its abrasive action on the opposing enamel. PURPOSE This study comparatively evaluated wear of enamel when opposed by three different surface finishes of ceramic. MATERIALS AND METHODS A total of 60 metal-ceramic discs (10 mm × 2 mm) with different surface finishes were fabricated. They were div...

متن کامل

بررسی اثر پالیش بر روی استحکام Flexural پرسلن فلدسپاتیک و مقایسه آن با اتوگلیز و اورگلیز

Statement of Problem: Ceramic restorations are popular because they can provide the most natural replacement for teeth. However, the brittleness of ceramics is a primary disadvantage. There are various methods for strengthening ceramics such as metal framework, ceramic cores, and surface strengthening mechanisms through glazing, work hardening and ion exchange. Purpose: The purpose of this stud...

متن کامل

مقایسه استحکام خمشی پرسلن دندانی جدید (D4 Dentin)  با پرسلن دندانی کارخانه Vita (VMK 68N)

Statement of Problem: Dental porcelain is one of the best materials ever used in dentistry. Excellent tissue compatibility, esthetics, very low solubility in oral fluids, high compressive strength, and the lowest bacterial plaque accumulation on the glazed porcelain are some of its advantages. Porcelain brittleness due to its low tensile strength, impact strength and the occlusal attrition of o...

متن کامل

In Vitro Effects of Four Porcelain Surface Treatment Methods on Adhesion of Lactobacilli Acidophilus

  Objective: Adhesion of Lactobacillus acidophilus (L. acidophilus) to dental porcelain surface may lead to gingival inflammation and secondary caries. Surface roughness is among the factors affecting this adhesion. The purpose of this study was to evaluate the effects of four different surface treatment methods on adhesion of L. acidophilus to dental porcelain.   Methods: Sixty specimens (3x10...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 4  شماره 

صفحات  -

تاریخ انتشار 2012