Buckling of Ge nanowires under uniaxial compression

نویسندگان

  • Qingyuan Meng
  • Yuhang Jing
چکیده

Molecular dynamics simulations are performed to investigate the buckling properties of [100]-, [110]-, [111]-, and [112]-oriented single-crystalline germanium nanowires under uniaxial compression. The effects of simulation temperature, strain rate, and wire length on the buckling behaviour are investigated. The simulation results indicate that critical load clearly decreases with increasing temperature and with decreasing strain rate. Additionally, the present results show that the critical load decreases with the increase of wire length, which is in agreement with the Euler theory.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Buckling Behavior of Composite Plates with a Pre-central Circular Delamination Defect under in-Plane Uniaxial Compression

Delamination is one of the most common failure modes in composite structures. In the case of in-plane compressional loading, delamination of a layered flat structure can cause a local buckling in delaminated area which subsequently affects the overall stiffness of the initial structure. This leads to an early failure of the overall structure. Moreover, with an increase in load, the delaminated ...

متن کامل

Rate dependent deformation of a silicon nanowire under uniaxial compression: Yielding, buckling and constitutive description

0927-0256/$ see front matter Crown Copyright 2 doi:10.1016/j.commatsci.2011.07.037 ⇑ Corresponding author. Address: Mechanical Engin of Mechanical and Manufacturing Engineering, The Un NSW 2052, Australia. Tel.: +61 2 9385 6078; fax: +61 E-mail address: [email protected] (L.C. This paper investigates the effect of compressive strain rate on the mechanical behaviour of single crystallin...

متن کامل

Knockdown factors for buckling of cylindrical and spherical shells subject to reduced biaxial membrane stress

Cylindrical shells under uniaxial compression and spherical shells under equi-biaxial compression display the most extreme buckling sensitivity to imperfections. In engineering practice, the reduction of load carrying capacity due to imperfections is usually addressed by use of a knockdown factor to lower the critical buckling stress estimated or computed without accounting for imperfections. F...

متن کامل

Multi-shell gold nanowires under compression

Deformation properties of multi-wall gold nanowires under compressive loading are studied. Nanowires are simulated using a realistic many-body potential. Simulations start from cylindrical fcc (111) structures at T = 0 K. After annealing cycles axial compression is applied on multi-shell nanowires for a number of radii and lengths at T = 300 K. Several types of deformation are found, such as la...

متن کامل

Improved Design Formulae for Buckling of Orthotropic Plates under Combined Loading

Simple, accurate buckling interaction formulae are presented for long orthotropic plates with either simply supported or clamped longitudinal edges and under combined loading that are suitable for design studies. The loads include 1) combined uniaxial compression (or tension) and shear, 2) combined pure inplane bending and 3) shear and combined uniaxial compression (or tension) and pure inplane...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2010