Low temperature chemical vapor deposition growth of b-SiC on (100) Si using methylsilane and device characteristics

نویسندگان

  • C. W. Liu
  • J. C. Sturm
چکیده

The growth properties of b-SiC on ~100! Si grown by rapid thermal chemical vapor deposition, using a single precursor ~methylsilane! without an initial surface carbonization step, were investigated. An optimun growth temperature at 800 °C was found to grow single crystalline materials. A simple Al Schottky barrier fabricated on n-type SiC grown on Si substrates exhibited a ‘‘hard’’ reverse breakdown of 13 V with a positive temperature coefficient of 2310 °C up to 120 °C, indicating an avalanche mechanism. A Pt Schottky barrier fabricated on n-type SiC grown on tilted Si substrates to improve the surface morphology exhibited a breakdown voltage of 59 V, with a negative temperature coefficient. From the analysis of the electrical field distribution, the breakdown probably occurred at interface defects between SiC and Si, as suggested by Raman spectroscopy. To investigate minority transport behavior, SiC/Si heterojunction bipolar transistors ~HBTs! were fabricated and compared to Si bipolar junction transistors. The collector currents of the SiC/Si HBTs were similar to those of Si control transistors, because both devices had the same base structures. Compared to Si control transistors, the base currents of SiC/Si HBTs increased. It seems that the interface defects between Si and SiC act as recombination centers to deplete back-injected holes, instead of being the barrier to stop hole currents, and thus to increase the base currents of SiC/Si HBTs. © 1997 American Institute of Physics. @S0021-8979~97!03921-2#

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Growth and photoluminescence of high quality SiGeC random alloys on silicon substrates

We report chemical vapor deposition growth of SiGeC layers on ^100& Si substrates. At the growth temperature of 550 °C, the C concentration as high as 2% can be incorporated into SiGe ~Ge content ; 25%! to form single crystalline random alloys by using low flow of methylsilane ~0.25 sccm! as a C precursor added in a dichlorosilane and germane mixture. For intermediate methylsilane flow ~0.5 scc...

متن کامل

Synthesis and Characterization of Nanocrystalline Silicon Carbide Thin Films on Multimode Fiber Optic by means 150 MHz VHF-PECVD

In recent years, a number of advantages such as modification of nano-crystalline thin films, the ability for low-temperature deposition processes, the controlling of process, as well as high efficiency and repeatability of process, were offered using plasma deposition technique [1]. Silicon carbide (SiC) as a leading candidate for the replacement of Silicon (Si) for hightemperature and power el...

متن کامل

Synthesis and Characterization of Nanocrystalline Silicon Carbide Thin Films on Multimode Fiber Optic by means 150 MHz VHF-PECVD

In recent years, a number of advantages such as modification of nano-crystalline thin films, the ability for low-temperature deposition processes, the controlling of process, as well as high efficiency and repeatability of process, were offered using plasma deposition technique [1]. Silicon carbide (SiC) as a leading candidate for the replacement of Silicon (Si) for hightemperature and power el...

متن کامل

Carbon nanotube array thermal interfaces for high-temperature silicon carbide devices

Multiwalled carbon nanotube (MWCNT) arrays have been directly synthesized from templated Fe2O3 nanoparticles on the C-face of 4H-SiC substrates by microwave plasma chemical vapor deposition (MPCVD), and the room-temperature thermal resistances of SiC-MWCNT-Ag interfaces at 69–345 kPa as well as the thermal resistances of SiCMWCNT-Ag interfaces up to 250 C (at 69 kPa) have been measured using a ...

متن کامل

Fluorinated SiC CVD

For the emerging semiconductor material silicon carbide (SiC) used in high power devices, chemical vapor deposition (CVD) is the most prominent method to create the electrically active SiC epitaxial layers in the device. The process of growing such epitaxial layers is to use a hydrocarbon and silane diluted in hydrogen flow through a hot chamber where chemical reactions take place in such a man...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 1997