Three polyphosphates were used as inhibitors for poly(vinyl chloride) (PVC) photodegradation. The polyphosphates were added to PVC at a concentration of 0.5% by weight. The PVC films (40 µm thickness) were irradiated at room temperature with ultraviolet (UV) light for up to 300 h. The changes in PVC films after irradiation were monitored by Fourier transform infrared spectroscopy, weight loss, viscosity-average molecular weight determination, and atomic force microscopy. These changes were very noticeable in the blank PVC films compared to the ones obtained when additives were used. The polyphosphates can inhibit the PVC photodegradation through direct absorption of UV light, interactions with PVC chains, and acting as radical scavengers.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Photodegradation of Poly ( caprolactone ) / Poly ( vinyl chloride ) Blend

The photodegradation of a 1:1 blend of poly (caprolactone) and poly(vinyl chloride) has been studied by following carbon dioxide emission during UV exposure. Similar measurements were made on poly(caprolactone) and poly(vinyl chloride) homopolymers prepared and irradiated in the same way. It was found that the blend gave lower CO2 emission than either of the two homopolymers, indicating that th...

متن کامل

Photostabilizing Efficiency of Poly(vinyl chloride) in the Presence of Organotin(IV) Complexes as Photostabilizers.

Three organotin complexes containing furosemide as a ligand (L), Ph₃SnL, Me₂SnL₂ and Bu₂SnL₂, were synthesized and characterized. Octahedral geometry was proposed for the Me₂SnL₂ and Bu₂SnL₂, while the Ph₃SnL complex has trigonal bipyramid geometry. The synthesized organotin complexes (0.5% by weight) were used as additives to improve the photostability of poly(vinyl chloride), PVC, (40 μm thic...

متن کامل

Effect of some additives on degradation of poly (vinyl chloride- co- vinyl

The thermal decomposition of 86 % vinyl chloride 14 % vinyl acetate copolymer wasstudied by the conductometry technique in the presence of nitrogen. The kinetics of stability andthermal degradation of vinyl chloride- co- vinyl acetate (PVC- co- PVAc) copolymer withcopper, copper oxide and tricalcium dicitrate (st) were investigated at various temperatures (150-180 oC ) in solution. The rate coe...

متن کامل

The Effect of Ultraviolet Irradiation on the Physicochemical Properties of Poly(vinyl Chloride) Films Containing Organotin(IV) Complexes as Photostabilizers.

Three organotin(IV) complexes containing ciprofloxacin as a ligand (Ph₃SnL, Me₂SnL₂ and Bu₂SnL₂; 0.5% by weight) were used as additives to inhibit the photodegradation of polyvinyl chloride films (40 µm thickness) upon irradiation with ultraviolet light (λmax = 313 at a light intensity = 7.75 × 10-7 ein dm-3 S-1) at room temperature. The efficiency of organotin(IV) complexes as photostabilizers...

متن کامل

Removal of Dilute Benzene in Water through Ionic Liquid/Poly(Vinyl Chloride) Membranes by Pervaporation

This paper focuses on the effects of the addition of an ionic liquid, 1-Allyl-3-butylimidazilium bis(trifluoromethane sulfonyl)imide ([ABIM]TFSI), which has a high affinity for benzene, into the poly(vinyl chloride) (PVC) membrane on the pervaporation characteristics of the removal of benzene from aqueous solutions of dilute benzene. When aqueous solutions of 100~500 ppm benzene were permeated ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Molecules

دوره 22 11  شماره 

صفحات  -

تاریخ انتشار 2017