OBJECTIVE The objective this work was to assess the friction coefficient between brackets and wires of different materials under conditions simulating the oral environment. MATERIAL AND METHODS Stainless steel (SS) and titanium-molybdenum alloy (TMA) wires of 0.019x0.025-in diameter (American Orthodontics) and polycarbonate bracket (American Orthodontics), ceramic bracket (American Orthodontics), and metal bracket (3M Unitek) with slots of 0.022x0.030-in were used. The friction coefficient was assessed by means of mechanical traction with the system immersed in artificial saliva. The mean roughness of both wire surface and bracket slots was evaluated by using a surface profilometer. RESULTS The system using TMA wire and polycarbonate bracket had the highest roughness (p<0.05). SS wire with ceramic bracket had the highest friction coefficient, whereas the use of metallic bracket yielded the lowest (p<0.05). However, it was observed a statistically significant difference in the system using TMA wire and ceramic bracket compared to that using TMA wire and polycarbonate bracket (p=0.038). CONCLUSIONS Ceramic brackets in association with SS wire should be judiciously used, since this system showed a high friction coefficient.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Galvanic Corrosion and Ion Release from Different Orthodontic Brackets and Wires in Acidic Artificial Saliva: Part I

&nbsp; Objective: Corrosion resistance is among the most important properties of metal alloys used in the oral cavity. Consumption of acidic foods reduces the salivary pH and intensifies the corrosion of brackets and orthodontic wires. This study aimed to compare electro galvanic corrosion of different orthodontic brackets and wires and determine the amount of ions released into acidic artifici...

متن کامل

Galvanic Corrosion of Orthodontic Brackets and Wires in Acidic Artificial Saliva: Part II

  Objective: Orthodontic wires should have high resistance against corrosion in the oral environment. Since the effect of pH on corrosion has been well recognized, this study sought to assess and compare the electrochemical corrosion of orthodontic brackets and wires of different brands in acidic artificial saliva.   Methods: This in vitro experimental study was conducted on 24 mandibular centr...

متن کامل

Galvanic Corrosion among Different Combination of Orthodontic Archwires and Stainless Steel Brackets

Introduction: The aim of this study was to assess the galvanic behavior of different bracket and archwire combinations that are commonly used in orthodontic treatments. Methods: Three types of orthodontic archwires with a diameter of 0.016×0.022 inch and 80 standard edgewise maxillary central incisor brackets were selected. Three groups consisted of different wire-bracket couples and one group ...

متن کامل

بررسی مقاومت اصطکاکی سیم نیکل تیتانیوم ارتودنسی در زوایای مختلف قرارگیری براکت و سیم

Background and Objective: Resistance to sliding is a combination of friction and binding. When the angle between the bracket and the wire exceeds the critical angle, binding occurs. The influence of angulation is confounding because of certain inherent physical characteristics of materials. The present study was carried out to evaluate the effect of wire- bracket angulation on resistance to sli...

متن کامل

Evaluation of the Effect of an Experimental Herbal versus Fluoridated Mouthwash on Frictional Resistance and Surface Roughness between Orthodontic Brackets and Two Types of Archwire: In Vitro Study

Introduction: The present study aimed to evaluate an experimental herbal mouthwash, as compared to sodium fluoride mouthwash on the frictional resistance and surface roughness between brackets and two rectangular archwire types. Methods: A total of 60 premolar׳s brackets engaged with 0.019×0.025 archwires made of stainless steel and nickel-titanium alloys were used in this study. The samples we...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 19  شماره 

صفحات  -

تاریخ انتشار 2011