The aim of this study was to characterize a conventional and a pressed porcelain for zirconia core as to biaxial flexural strength (BFS), apparent fracture toughness (FT) and microstructure composition, and to investigate the effect of glaze cooling rate on the BFS of the zirconia/porcelain bilayers. Monolayers of conventional porcelain Vita VM9 and pressed porcelain Vita PM9 (n=15) (12 mm diameter x 1.2 mm thick) were prepared for the BFS test (MPa). Apparent fracture toughness (MPa.m1/2) was measured by indentation technique (n=15). t-Student test was performed for statistical analysis. Scanning electron microscopy and x-ray diffraction were used to analyze the porcelain's microstructure. For the BFS of bilayers, zirconia discs (12 mm diameter x 1 mm thick) (Vita In-Ceram YZ) were veneered with the two porcelains (1 mm thick). After the glaze firing simulation, the specimens were submitted to fast or slow cooling (n=15). Apparent fracture toughness (MPa.m1/2) was measured on the porcelain surface of bilayers (n=15) and residual stress was calculated. Two-way ANOVA (porcelain and cooling method) was used for the bilayer analysis (a=0.05). Vita PM9 monolayer exhibited significantly higher BFS (p<0.01), but there was no significant difference (p=0.41) in the FT between the porcelains. For bilayer specimens, the two-way ANOVA for BFS was significant for the porcelain variable only (p<0.01) better for Vita PM9/zirconia. Two-way ANOVA for the FT for the bilayers was not significant for any variable. All groups showed compressive residual stresses. The pressed porcelain seems to be mechanically more effective for zirconia veneering.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Influence of Veneering Fabrication Techniques and Gas-Phase Fluorination on Bond Strength between Zirconia and Veneering Ceramics.

PURPOSE Porcelain chipping has been one of the main problems of porcelain-fused-to-zirconia restorations. This study evaluates the bond strengths of layered, pressed, and adhesively bonded porcelain to yttria-stabilized zirconia substrates that have undergone traditional preparation or gas-phase fluorination. MATERIALS AND METHODS A three-point bending test was used to evaluate the bond stren...

متن کامل

Low-Fusing Porcelain Glaze Application on 3Y-TZP Surfaces can Enhance Zirconia-Porcelain Adhesion.

The aim of this study was to assess whether surface treatment improves zirconia-porcelain adhesion. The 3Y-TZP blocks were cut into squares, then polished and sintered. The zirconia surface treatments were performed as follows: no treatment (C); tribochemical silica coating (TBS); glaze application + hydrofluoric acid etching (GA); glaze application + hydrofluoric acid etching + silanization (G...

متن کامل

Effects of extreme cooling methods on mechanical properties and shear bond strength of bilayered porcelain/3Y-TZP specimens.

OBJECTIVES This study investigated the effect of extreme cooling methods on the flexural strength, reliability and shear bond strength of veneer porcelain for zirconia. METHODS Vita VM9 porcelain was sintered on zirconia bar specimens and cooled by one of the following methods: inside a switched-off furnace (slow), at room temperature (normal) or immediately by compressed air (fast). Three-po...

متن کامل

Dental Porcelain (Core) with Improved Fracture Toughness and Microhardness

To study the effect of different cooling rates after glaze firing on Radius of radial crack, Fracture toughness and Microhardness of Alumina reinforced porcelain. Total 30 porcelain discs reinforced with aluminium oxide of 8mm diameter×0.6mmthickness were prepared. Specimens were divided into three groups, each group containing ten discs. They were positioned at the entrance of the furnace with...

متن کامل

Effect of cooling rate on shear bond strength of veneering porcelain to a zirconia ceramic material.

The purpose of the present study was to evaluate the effect of cooling rates after firing procedures of veneering porcelain on shear bond strength between veneering porcelain and a zirconium dioxide (zirconia; ZrO₂) ceramic material. A total of 48 ZrO₂ disks were divided equally into three groups. Two veneering porcelains that are recommended for ZrO₂ material - Cerabien ZR (CZR), IPS e.max Cer...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Brazilian dental journal

دوره 27 5  شماره 

صفحات  -

تاریخ انتشار 2016