Fractographic Aspects of Stress Corrosion Failure of Zircaloy 2 in CH3OH HCL Solutions

author

Abstract:

Fracture surface of Zircaloy-2 specimens tested under constant crosshead speed in CH3OH/0.4 Vol. %HCI solution with and without selenium (25 ppm) addition was studied. Using a combined process of deformation and annealing, coarse grained material was also obtained and examined. Two modes of stress corrosion crack propagation were observed: an intergranular zone caused by stress assisted anodic dissolution, and a transgranular cleavage zone, due to hydrogen absorption.

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

AN INVESTIGATION ON CORROSION BEHAVIOUR OF A356-10 VOL.% SiC COMPOSITES IN HCl SOLUTIONS

In this study, corrosion behaviour of A356-10 vol.% SiC composites casted by gravity and squeeze casting is evaluated. For this purpose, prepared samples were immersed in HCl solution for 1h at open circuit potential. Tafel polarization and electrochemical impedance spectroscopy (EIS) were carried out to study the corrosion resistance of composites. The Tafel polarization and EIS studies of ...

full text

INHIBITION OF CORROSION OF CARBON STEEL IN HCl SOLUTIONS BY VARIOUS SCHIFF BASE

Evaluation of corrosion inhibitors for steel in acidic media is important for some industrial facilities as well as is very interesting from theoretical aspects. Most of the effective inhibitors are organic compounds containing nitrogen, phosphorus and sulphur in their structures [1, 2]. Heteroatoms such as nitrogen, oxygen and sulphur are capable of forming coordinate covalent bond with metal ...

full text

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 3  issue 1

pages  23- 30

publication date 1990-05-01

By following a journal you will be notified via email when a new issue of this journal is published.

Keywords

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023