Investigation of the Heat Treatment Effect on Microstructures and Phases of Inconel 713C Superalloy

author

  • Mahboobeh Azadi Material Eng., Semnan University, Faculty of Material and metallurgical engineering
Abstract:

The application of Inconel 713C is very vast in different industries such as in automobiles, aircrafts, boilers and turbines. In this paper, Inconel 713C specimens were solutionized at 1000 and 1200 °C for 1 hours in order to study changes in phases and the structure of alloy to modify the γ' phase. The optical and the scanning electron microscopy were used to investigate the structure and the energy dispersive spectroscopic (EDS) and the X-ray diffraction (XRD) were applied to identify the composition and phase changes. Results showed that the solutioning heat treatment at 1000 °C for 1 hour caused to participate Cr23C6, but when the temperature of heat treatment increased to 1200°C, chromium carbides solutionized in the γ matrix. Besides, by applying the heat treatment at temperature of 1000 °C, the γ' phase dissolved in (200) and (220) plane and this phase in the plane of (111) had the best stability. However the (220) plane of γ' phase was stable thermodynamically for the specimen without the heat treatment. Phases of Ni5Al3 and Al0.42Ni0.58 were observed at the temperatures of 1000 and 1200 °C, respectively. In addition, as the heat treatment temperature increased from 1000 to 1200 °C the new phase of AlNi3C0.5 solutionized in the γ matrix.

Download for Free

Sign up for free to access the full text

Already have an account?login

similar resources

an investigation of the impact of self monitoring on langauge teachers motivational practice and its effect on learners motivation

the central purpose of this study was to conduct a case study about the role of self monitoring in teacher’s use of motivational strategies. furthermore it focused on how these strategies affected students’ motivational behavior. although many studies have been done to investigate teachers’ motivational strategies use (cheng & d?rnyei, 2007; d?rnyei & csizer, 1998; green, 2001, guilloteaux & d?...

the effect of task complexity on lexical complexity and grammatical accuracy of efl learners’ argumentative writing

بر اساس فرضیه شناخت رابینسون (2001 و 2003 و 2005) و مدل ظرفیت توجه محدود اسکهان (1998)، این تحقیق تاثیر پیچیدگی تکلیف را بر پیچیدگی واژگان و صحت گرامری نوشتار مباحثه ای 60 نفر از دانشجویان زبان انگلیسی بررسی کرد. میزان پیچیدگی تکلیف از طریق فاکتورهای پراکندگی-منابع تعیین شد. همه ی شرکت کنندگان به صورت نیمه تصادفی به یکی از سه گروه: (1) گروه موضوع، (2) گروه موضوع + اندیشه و (3) گروه موضوع + اندی...

15 صفحه اول

the effect of taftan pozzolan on the compressive strength of concrete in the environmental conditions of oman sea (chabahar port)

cement is an essential ingredient in the concrete buildings. for production of cement considerable amount of fossil fuel and electrical energy is consumed. on the other hand for generating one tone of portland cement, nearly one ton of carbon dioxide is released. it shows that 7 percent of the total released carbon dioxide in the world relates to the cement industry. considering ecological issu...

My Resources

Save resource for easier access later

Save to my library Already added to my library

{@ msg_add @}


Journal title

volume 30  issue 10

pages  1538- 1544

publication date 2017-10-01

By following a journal you will be notified via email when a new issue of this journal is published.

Hosted on Doprax cloud platform doprax.com

copyright © 2015-2023