An Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution
نویسندگان
چکیده مقاله:
The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and also the possibility of crack initiation. Based on the obtained results, it was found that the corrosion rate increased in concentrated amine solutions. Also, by increasing temperature from 25 to 70 °C both corrosion rate and susceptibility to SCC initiation were intensified. Increment of amine concentration and also increase in temperature led to more absorption of CO2, generating a more acidic solution. Overall it could be stated that while for the grade 430 stainless steel investigated in this study corrosion and cracking was observed Therefore it could be concluded that in amine-containing environments this steel is not a very suitable alternative for carbon steels, which are commonly used in these environments.
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
An Outrun Competition of Corrosion Fatigue and Stress Corrosion Cracking on Crack Initiation in a Compressor Blade
First row rotating blades of four axial-flow compressors were prematurely fractured. Previous investigations showed that the site atmosphere contains corrosive compounds which lead to an increase in possibility of pitting on the blades. It was also revealed that the crack was originated from two corrosion pits. Thus, this work is conducted to ascertain which of fatigue or stress corrosion crack...
متن کاملStress Corrosion Cracking of an Austenitic Stainless Steel in Nitrite-Containing Chloride Solutions
This article describes the susceptibility of 316L stainless steel to stress corrosion cracking (SCC) in a nitrite-containing chloride solution. Slow strain rate testing (SSRT) in 30 wt. % MgCl₂ solution established SCC susceptibility, as evidenced by post-SSRT fractography. Addition of nitrite to the chloride solution, which is reported to have inhibitive influence on corrosion of stainless ste...
متن کاملA Continuum Damage Model for the Stress Corrosion Cracking of Austenitic Stainless Steel
In the present work, the mechanical behavior of stress corrosion cracking phenomenon is described. Such phenomenon presents strong complexity due to metallurgic and electrochemical aspects. A methodology for modeling both SSR (Slow Strain Rate) and CL (Constant Load) tests based upon thermodynamics of continuum solids and elastoplastic damage is proposed. In this macroscopic approach, besides t...
متن کاملExternal corrosion resistance of steel and ferritic stainless steel exhaust systems
The exhaust system has a number of requirements to fulfil. The major ones are to reduce the noise level created by the engine, to channel the waste gases out the rear of the automobile, to minimize the reduction in engine performance, and to have an acceptable service life and cost1. The exhaust system is divided into two main parts, the hot end and the cold end. The components comprising the h...
متن کاملStainless steel pitting and early-stage stress corrosion cracking under ultra-low elastic load
متن کامل
Stress Corrosion Crack Growth Mechanism on SUS316L Stainless Steel
The stress corrosion cracking (SCC) of stainless steel is one of the biggest problems for maintaining atomic power and chemical plants. However the mechanism has not been solved because of difficulty in observing hydrogen movement. In order to solve this problem, the author has developed a new SCC test method that enables the super Kelvin force microscope (SKFM) and the Kelvin force microscope ...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 53 شماره 2
صفحات 203- 210
تاریخ انتشار 2019-12-01
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023