First row rotating blades of four axial-flow compressors were prematurely fractured. Previous investigations showed that the site atmosphere contains corrosive compounds which lead to an increase in possibility of pitting on the blades. It was also revealed that the crack was originated from two corrosion pits. Thus, this work is conducted to ascertain which of fatigue or stress corrosion cracking (SCC) mechanisms was predominant in transition of pits into initial cracks. To this end, experimental, numerical and theoretical studies are considered. Scanning Electron Microscope (SEM) and fractography of the broken blade indicate that the pits join together and make one bigger pit under SCC mechanism which reduces the failure time. 3-D models of the pitting on the blade under existing forces are analyzed by ABAQUS software. The simulation results show the location of maximum stress concentration inside one of the pits which is compatible with the location of initial SCC crack. Theoretical analysis shows stress intensity range around the pits smaller than threshold stress intensity range; thus, cracks initiated and propagated at the mouth of the pits under SCC mechanism. Then the pits join together and make one equivalent pit, so that stress intensity range reaches to threshold stress intensity range and finally crack propagates under fatigue mechanism.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

An Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution

The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and ...

متن کامل

Tarnish Resistance, Corrosion and Stress Corrosion Cracking of Gold Alloys

Tarnishing, corrosion and stress corrosion cracking (SeC) of gold alloys are related phenomena. They present problems when they occur in gold jewellery, dental gold alloys and electronic devices. They are exploited, however, in the depletion gilding and finishing of gold jewellery; and in the extraction, refining and fire assaying of gold. There is still much that is not known about these pheno...

متن کامل

Fatigue Analysis of Crack Growing Rate and Stress Intensity Factor for Stress Corrosion Cracking in a Pipeline System

Environment-assisted cracking (EAC) is one of the most serious causes of structural failure over a broad range of industrial applications including offshore structures. In EAC condition there is not a definite relation such as Paris equation in Linear Elastic Fracture Mechanics (LEFM). According to studying and searching a lot what the researchers said either a material has contact with hydroge...

متن کامل

Corrosion Product Film-Induced Stress Facilitates Stress Corrosion Cracking

Finite element analyses were conducted to clarify the role of corrosion product films (CPFs) in stress corrosion cracking (SCC). Flat and U-shaped edge-notched specimens were investigated in terms of the CPF-induced stress in the metallic substrate and the stress in the CPF. For a U-shaped edge-notched specimen, the stress field in front of the notch tip is affected by the Young's modulus of th...

متن کامل

ARPA Coupling Program on Stress - Corrosion Cracking

A progress report of the ret arch invest carried out on the problem of stress-cor high strength materials under ARPA Order Work at Carnegie-Mellon University, Lehi Georgia Institute of Technology, The Boe American University, and the Naval Resea cerning test techniques, materials chara metallurgy, surface studies, and corrosi described. The report is divided into t covering work on high strengt...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 27  شماره 5

صفحات  785- 792

تاریخ انتشار 2014-05-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023