Effect of Opaque Porcelain Thickness Bond Strength of Porcelain to Ni-Cr Alloys

نویسندگان

  • Farhood Massoumi
  • Akram Mossaei
چکیده مقاله:

Objectives: Metal-ceramic restorations are the standard by which all esthetic restorations are measured. Fracture of dental restorations is a multifactorial problem, which is serious and costly. Debonding of porcelain from metal substructure and the bond strength depend on many factors. The purpose of this study was to determine whether or not the opaque porcelain thickness has a significant effect on metal ceramic bond strength utilizing the ISO 9663 standard crack initiation test. Methods: Thirty rectangular Ni-Cr metal bars (25x5x0.3mm) were fabricated according to ISO9663 standards. The metal bars were divided into 3 groups of 10. Opaque, body and enamel Noritake porcelain were applied on the middle of the bar according to ISO9663 standards up to 1mm porcelain thickness. The opaque porcelain thicknesses were 0.1, 0.2, and 0.3 mm, respectively in the 3 groups. The 3-point bending test was applied according to the ISO9663 standards and Ffail was measured using a universal testing machine with across head speed of 1.5mm/min. Results: Analyses of the raw data by one-way ANOVA demonstrated no significant differences among the three experimental groups (P=0.26).[th1] [A2]  Conclusion: Within the limitations of this study, it is concluded that 0.1mm opaque porcelain provides sufficient bond strength between metal and ceramic in metal-ceramic restorations  [th1]مقدار دقیق  pvalue گزارش شود.  [A2]انجام شد.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Comparison of the Effect of Three methods of Porcelain Surface Treatment on Shear Bond Strength of Composite to Porcelain

Background and Aim: Several methods are available for intraoral repair of chipped porcelain restorations by composite resin. Also, there is still controversy regarding the best method of porcelain repair in terms of bond strength and cost effectiveness. This study aimed to compare three methods of porcelain surface treatment on shear bond strength (SBS) of composite to porcelain. Materials a...

متن کامل

Comparison of the Effect of Nd:YAG Laser and Sandblasting on Shear Bond Strength of a Commercial Ni-Cr Alloy to Porcelain

Introduction: Failures might occur at metal‒porcelain interfaces as a problem with metal‒ceramic restorations even with the application of airborne-particle abrasion technique. This study was undertaken to evaluate the effect of Nd:YAG laser treatment on the bond strength of porcelain fused to metal. Methods:  Twenty-four cylindrical specimens (4 mm in diameter and 4 mm in height) were made of ...

متن کامل

Laboratory evaluation of shear bond strength of porcelain repair methods

Introduction: Porcelain fracture is a relatively common problem in clinical dental practice. Various methods have been proposed for repairing porcelain fractures including direct composite resin repair or construction of a porcelain laminate veneer and its cementation with a resin cement. Evaluation of shear bond strength of porcelain repair methods was the purpose of this study. Methods: Tw...

متن کامل

Effect of casting atmosphere on the shear bond strength of a ceramic to Ni-Cr and Ni-Cr-Be alloys.

The success of metal-ceramic restorations depends on an optimal bond between metal and ceramic. This study evaluated the effect of 3 casting atmospheres on the metal-ceramic bond strength (MCBS) of 2 Ni-Cr alloys, with beryllium (Fit Cast V) and without beryllium (Fit Cast SB). Sixty acrylic resin patterns (8 mm long and 5 mm diameter) were obtained using a fluorocarbon resin matrix. Wax was us...

متن کامل

Effects of surface treatments and cement types on the bond strength of porcelain-to-porcelain repair.

PURPOSE The purpose of this in vitro study was to evaluate the effects of four surface treatments and two resin cements on the repair bond strength of a ceramic primer. MATERIALS AND METHODS Eighty-eight pairs of disks (10 and 5 mm in diameter, 3 mm thickness) were prepared from heat-pressed feldspar ceramics (GC Initial IQ). After being stored in mucin-artificial saliva for 2 weeks, the 10-m...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 34  شماره None

صفحات  72- 81

تاریخ انتشار 2016-06

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

کلمات کلیدی

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023