Production of aluminum matrix composites is widespread because these material provide enhanced mechanical properties compared to aluminum. One the most important parameters of metal matrix composite production is uniform distribution of reinforcing nanoparticles in matrices using the stir-casting method. Second is ensuring high wettability, which is determined by evaluating the properties of materials on a nano-scale. In this study, aluminum composites were reinforced with titanium carbide nanoparticles coated with aluminum to increase wettability. Particles were prepared and added to a molten aluminum alloy. After stirring the particle mixture as a variable parameter, casting was conducted in a sand mold. To evaluate the mechanical properties of the composite, the Brinell test was used to determine hardness and the pin-on-disk test was used to measure wear rate and the friction coefficient. The results showed that the hardness of the composite increased from 84 BHN to 134 BHN as nanoparticles were added to the alloy. Additionally, as stirring time increased, weight loss decreased with respect to the base alloy, while the coefficient of friction increased.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Enhancing Wear Resistance of Squeeze Cast AC2A Aluminum Alloy

The effect of squeeze casting process parameters on wear behavior of AC2A aluminium alloy was primarily investigated in this experimental study. Five process parameters, namely squeeze pressure, pouring temperature, die temperature, die material and compression time, each at four levels were chosen and sixteen experimental runs based on L16 orthogonal array were performed. From analysis of vari...

متن کامل

Marginal and internal adaptation of commercially pure titanium and titanium-aluminum-vanadium alloy cast restorations.

AIM The purpose of this in vitro study was to investigate the marginal accuracy and internal fit of complete cast crowns and three-unit fixed partial dentures (FPDs) cast with commercially pure titanium (CPTi) and Titanium-Aluminum-Vanadium alloy (Ti-6Al-4V). METHODS AND MATERIALS CPTi and Ti-6Al-4V alloy were used to cast twelve single crowns and twelve three-unit FPDs. A traveling microscop...

متن کامل

Evaluation of Flank Wear of Iron-rich Binder Carbide Cutting Tool in Turning of Titanium Alloy

Despite the fact that Titanium material has been considered as difficult to cut material, its usage has been increasing day by day in all engineering sectors; wherever criticality is encountered. Many studies are going on in view of increasing tool life at high cutting speed to improve productivity. In this study, attempt has been made to see the effect of iron as a partial substitution  along ...

متن کامل

Vickers hardness of cast commercially pure titanium and Ti-6Al-4V alloy submitted to heat treatments.

The purpose of this study was to evaluate the effect of heat treatments on the Vickers hardness of commercially pure titanium and Ti-6Al-4V cast alloys. Six-millimeter-diameter cylindrical specimens were cast in a Rematitan System. Commercially pure titanium and Ti-6Al-4V alloy specimens were randomly assigned to 3 groups (n=10) that received the following heat treatments: control (no heat trea...

متن کامل

Friction stir welding of dissimilar joint of aluminum alloy 5083 and commercially pure titanium

In this study, commercially pure titanium and aluminum alloy 5083 in connection rotational speed of 1120 rpm and a feed rate of 50 mm per minute for butt welding by friction stir welding has been successfully completed. Micro-structure, hardness and tensile test was conducted on the connection. Welding area is a composite of aluminum and titanium particles that the particles plays an important ...

متن کامل

Friction stir welding of dissimilar joint of aluminum alloy 5083 and commercially pure titanium

In this study, commercially pure titanium and aluminum alloy 5083 in connection rotational speed of 1120 rpm and a feed rate of 50 mm per minute for butt welding by friction stir welding has been successfully completed. Micro-structure, hardness and tensile test was conducted on the connection. Welding area is a composite of aluminum and titanium particles that the particles plays an important ...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 5  شماره 1

صفحات  75- 81

تاریخ انتشار 2018-04-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023