Laboratory evaluation of shear bond strength of porcelain repair methods

نویسندگان

  • Abdolhamid Alhavaz ,Department of Prosthodontics, Dental Materials Research Center, Faculty of Dentistry, Babol University of Medical Sciences, Babol-Iran.
  • Pouya Aslani ,Faculty of Dentistry, Babol University of Medical Sciences, Babol-Iran.
  • Vahid Soltankarimi ,Department of Prosthodontics, Faculty of Dentistry, Babol University of Medical Sciences, Babol-Iran.
چکیده مقاله:

Introduction: Porcelain fracture is a relatively common problem in clinical dental practice. Various methods have been proposed for repairing porcelain fractures including direct composite resin repair or construction of a porcelain laminate veneer and its cementation with a resin cement. Evaluation of shear bond strength of porcelain repair methods was the purpose of this study. Methods: Twenty feldspathic porcelain discs (10 mm in diameter) were fabricated. The samples underwent air-born abrasion with an aluminum oxide and etching with HF, and were then ultrasonically cleaned and randomized into two groups: 1- repair with porcelain disc (7 mm in diameter) with light cure cement (Choice 2) and 2- repair with resin composite (Clearfil AP-X). We measured the shear bond strength of the samples by Zwick Roll at 0.5 mm/min crosshead speed.  Results: The resin composite group had the highest shear bond strength (12.91 MPa). We found no significant differences between the choice and composite groups (p=0.970). Conclusions: Our findings indicate that resin composite yields acceptable shear bond strength to be used in porcelain repair.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Silane on Shear Bond Strength of Two Porcelain Repair Systems

Objectives: Ceramics have advantages such as optimal esthetics and biocompatibility. However, in the oral environment, they are subjected to high levels of stress due to masticatory forces, saliva, thermal changes and alterations of pH, which increase their risk of fracture. Since replacement of these restorations is costly and time-consuming, composite resin is often used for intraoral repair ...

متن کامل

Comparison of the Effect of Three methods of Porcelain Surface Treatment on Shear Bond Strength of Composite to Porcelain

Background and Aim: Several methods are available for intraoral repair of chipped porcelain restorations by composite resin. Also, there is still controversy regarding the best method of porcelain repair in terms of bond strength and cost effectiveness. This study aimed to compare three methods of porcelain surface treatment on shear bond strength (SBS) of composite to porcelain. Materials a...

متن کامل

Shear strength of the composite bond to etched porcelain.

The shear bond strength of composite resin to porcelain was investigated to optimize variables for bonding porcelain laminate veneers. Scanning electron microscopy was initially used to examine the surface configuration of porcelain prepared under various conditions. A factorial experiment was undertaken to determine the effects of three different bonding methods on both etched and non-etched p...

متن کامل

Shear bond strength of veneering porcelain to porous zirconia.

In this study, two types of porous zirconia and dense zirconia were used. The flexural strength of non-layered zirconia specimens and those of the layered zirconia specimens with veneering porcelain were examined. Furthermore, the shear bond strength of veneering porcelain to zirconia was examined. The flexural strength of the non-layered specimens was 1,220 MPa for dense zirconia and 220 to 30...

متن کامل

Shear bond strength of composite resin to porcelain.

This study evaluated the effect of porcelain surface treatment on the shear bond strength of composite resin to various porcelains and porcelain combinations. A variety of feldspathic porcelains with low and medium alumina content were tested. Porcelain/composite resin samples were stored in 37 degrees C water, thermocycled 1,000 times, and tested in shear. A 3-minute etching using hydrofluoric...

متن کامل

effect of silane on shear bond strength of two porcelain repair systems

objective: ceramics have advantages such as optimal esthetics and biocompatibility. however, in the oral environment, they are subjected to high levels of stress due to masticatory forces, saliva, thermal changes and alterations of ph, which increase their risk of fracture. since replacement of these restorations is costly and time-consuming, composite resin is often used for intraoral repair o...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 1  شماره None

صفحات  14- 18