ON THE FORMATION OF STRAY GRAINS IN DIRECTIONALLY-SOLIDIFIED NI-BASED SUPERALLOYS WITH VARYING CROSS SECTIONS
نویسندگان
چکیده مقاله:
Formation of stray grain defects particularly around re-entrant features of the turbine blade airfoils is one of the major problems in directional and single crystal solidification processes. In this work, directional solidification tests of the GTD-111 Ni-based superalloy were conducted at different withdrawal velocities of 3, 6 and 9 mm.min-1 using various stepped cylindrical and cubic designs. The process was also simulated using ProCAST finite element solver to characterize the crystal orientations. The phase transformation temperatures of the superalloy were estimated by the differential scanning calorimetry test. A process map was developed to predict the formation of stray grains in the platform regions of the stepped cylindrical and cubic specimens using the experimentally-validated simulation model. The process map shows critical values of the platform size, withdrawal velocity and initial sample size for the stray grain formation. The withdrawal velocity, platform size and initial sample size all had an inverse effect on the formation of stray grains.
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
A Thermomechanical Fatigue Crack Initiation Model for Directionally-solidified Ni-base Superalloys
Nickel-base superalloys have been used extensively in power generation applications due to their high strength at temperatures up to 1093°C. When the material is subjected to complex mechanical loading superimposed with thermal loading, fatigue interacts with either creep and/or oxidation. Directionallysolidified (DS) materials are often used in place of polycrystalline (PC) materials since the...
متن کاملFreckle Defect Formation near the Casting Interfaces of Directionally Solidified Superalloys
Freckle defects usually appear on the surface of castings and industrial ingots during the directional solidification process and most of them are located near the interface between the shell mold and superalloys. Ceramic cores create more interfaces in the directionally solidified (DS) and single crystal (SX) hollow turbine blades. In order to investigate the location of freckle occurrence in ...
متن کاملThermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy
A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...
متن کاملPrecipitation in a Ni - Al - Mo Directionally Solidified Eutectic Composite
The most recently developed high temperature materials are known as in-situ composites or directionally solidified eutectics. Since the composites are formed during solidification, they have excellent morphological stabilities up to near their melting temperatures. The Ni-Al-Mo system has received the greatest attention for recent several years(1)~(3) since the alloy is expected to form a struc...
متن کاملEffect of pre-exposure on crack initiation life of a directionally solidified Ni-base superalloy
Article history: Received 6 February 2008 Received in revised form 1 July 2008 Accepted 24 July 2008 Available online 5 August 2008
متن کاملOn oscillatory microstructure during cellular growth of directionally solidified Sn–36at.%Ni peritectic alloy
An oscillatory microstructure has been observed during deep-cellular growth of directionally solidified Sn-36at.%Ni hyperperitectic alloy containing intermetallic compounds with narrow solubility range. This oscillatory microstructure with a dimension of tens of micrometers has been observed for the first time. The morphology of this wave-like oscillatory structure is similar to secondary dendr...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 14 شماره 4
صفحات 12- 24
تاریخ انتشار 2017-12
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023