The Inhibition Effect of Polyethylenimine (PEI) on Pitting Corrosion of 304 Austenitic Stainless Steel in 3.5% NaCl Solution
نویسندگان
چکیده مقاله:
One of the problems in the case of stainless steels is their low corrosion resistance against pitting corrosion in chloride containing environments, thereby leading to severe damage to industries. In this research, the pitting corrosion of 304 austenitic stainless steel was studied in 3.5% NaCl solution at room temperature (25˚C) by performing electrochemical measurements (containing cyclic polarization and electrochemical impedance spectroscopy) and immersion measurements. Moreover, the effect of adding different concentrations of PEI inhibitor with two mean molar masses (2000 and 60,000 g/mol) on pitting corrosion was investigated. Finally, the adsorption behavior of this inhibitor on the alloy surface was investigated by ATR-FT.IR and AFM methods. It was observed that both inhibitors prevented uniform and pitting corrosion successfully, but PEI (60,000 g/mol) had better inhibition efficiency than PEI (2000 g/mol).
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
the inhibition effect of polyethylenimine (pei) on pitting corrosion of 304 austenitic stainless steel in 3.5% nacl solution
one of the problems in the case of stainless steels is their low corrosion resistance against pitting corrosionin chloride containing environments, thereby leading to severe damage to industries. in this research, the pitting corrosion of 304 austenitic stainless steel was studied in 3.5% nacl solution at room temperature (25˚c) by performing electrochemical measurements (containing cyclic pola...
متن کاملIMPROVING PITTING CORROSION OF 304 STAINLESS STEEL BY ELECTROPOLISHING TECHNIQUE
Several surface modification techniques such as ion implantation, surface laser melting, have been employed to improve pitting corrosion resistance of stainless steel. Electropolishing is a technique in which the surface roughness is eliminated through a selective electrochemical dissolution. The effect of electropolishing on pitting corrosion of 304 stainless steel (SS) was investigated employ...
متن کاملInhibition Effect of 2,2’-bipyridyl on the Corrosion of Austenitic Stainless Steel in 0.5M H2SO4
The corrosion inhibition of AISI309 austenitic stainless steel by 2,2'-Bipyridyl in 0.5M H 2 SO 4 at 298K was studied using the mass loss’ method, the potentiodynamic polarization (Tafel), the linear polarization (LRP) and the electrochemical impedance spectroscopy (EIS). The results showed a mixed inhibition mode and an increase in the charge transfer resistance, due to inhibitor molecules’ ad...
متن کاملEffect of Crystallographic Orientation on the Pitting Corrosion Resistance of Laser Surface Melted AISI 304L Austenitic Stainless Steel
The localized corrosion behavior of laser surface melted 304L austenitic stainless steel was studied by potentiodynamic polarization test. The extent of improvement in corrosion resistance was governed by the preferred orientation and the percentage of delta ferrite present on the surface of the laser melted sample. It was established by orientation imaging microscopy that the highest pitting p...
متن کاملGrain Size Effect on the Hot Deformation Processing Map of AISI 304 Austenitic Stainless Steel
In this study, the hot deformation processing map of AISI 304 austenitic stainless steel in two initial grain sizes of 15 and 40 μm was investigated. For this purpose, cylindrical samples were used in the hot compression test at the temperature range of 950-1100 °C and the strain rate of 0.005-0.5% s-1. At first, the relationship between the peak stress and Zener-Hollomon parameter w...
متن کاملEffect of nitriding temperature on the nanostructure and corrosion properties of Nickel coated 304 stainless steel
Nickel films of 150 nm thickness were deposited on 304 stainless steel and post annealed under flow of nitrogen at different temperatures. The prepared samples were corrosion tested in 1.0 M H2SO4 solution using potentiodynamic polarization technique. Crystallographic and morphological structure of the samples were analysed by X-ray diffraction XRD and atomic force microscopy AFM respectively b...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 10 شماره 1
صفحات 14- 22
تاریخ انتشار 2013-07-01
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023