Boriding of In-738 Superalloy via the Pack Cementation Method and the Study of the Kinetic of Boride Layer Formation
نویسندگان
چکیده مقاله:
In this study, mechanism and kinetic of formation of boride layer on In-738 superalloy were investigated via diffusion pack cementation method. Boriding was carried out at 900 °C for several short times (5, 15, 45 and 60 min). Phase study by means of X Ray defragtion (XRD) indicated that in addition to Ni3B, other phases such as Cr5B3, AlB2, and W2B were formed at the first period of process, and other compounds such as MoB2, VB, TiB, Ni6Si2B, and Mo2NiB2 were generated in the more prolonged time. SEM study also showed that not only the thickness of boride coating was increased, but also an interdiffusion zone (IDZ) was formed under the coating and it was grown by the upward diffusion of alloy elements. The kinetic study was good according to diffusion theory, confirming the two diffusion steps for IDZ. Thickness and hardness of the boride coating over 60 min process were 27.8 µm and 853 HV, respectively.
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
formation and evolution of regional organizations: the case study of the economic cooperation organization (eco)
abstract because of the many geopolitical, geo economical and geo strategically potentials and communicational capabilities of eco region, members can expand the convergence and the integration in base of this organization that have important impact on members development and expanding peace in international and regional level. based on quality analyzing of library findings and experts interv...
15 صفحه اولstudy of cohesive devices in the textbook of english for the students of apsychology by rastegarpour
this study investigates the cohesive devices used in the textbook of english for the students of psychology. the research questions and hypotheses in the present study are based on what frequency and distribution of grammatical and lexical cohesive devices are. then, to answer the questions all grammatical and lexical cohesive devices in reading comprehension passages from 6 units of 21units th...
the analysis of the role of the speech acts theory in translating and dubbing hollywood films
از محوری ترین اثراتی که یک فیلم سینمایی ایجاد می کند دیالوگ هایی است که هنرپیش گان فیلم میگویند. به زعم یک فیلم ساز, یک شیوه متأثر نمودن مخاطب از اثر منظوره نیروی گفتارهای گوینده, مثل نیروی عاطفی, ترس آور, غم انگیز, هیجان انگیز و غیره, است. این مطالعه به بررسی این مسأله مبادرت کرده است که آیا نیروی فراگفتاری هنرپیش گان به مثابه ی اعمال گفتاری در پنج فیلم هالیوودی در نسخه های دوبله شده باز تولید...
15 صفحه اولwuthering heights and the concept of marality/a sociological study of the novel
to discuss my point, i have collected quite a number of articles, anthologies, and books about "wuthering heights" applying various ideas and theories to this fantastic story. hence, i have come to believe that gadamer and jauss are rightful when they claim that "the individaul human mind is the center and origin of all meaning," 3 that reading literature is a reader-oriented activity, that it ...
15 صفحه اولa case study of the two translators of the holy quran: tahereh saffarzadeh and laleh bakhtiar
بطورکلی، کتاب های مقدسی همچون قران کریم را خوانندگان میتوان مطابق با پیش زمینه های مختلفی که درند درک کنند. محقق تلاش کرده نقش پیش زمینه اجتماعی-فرهنگی را روی ایدئولوژی های مترجمین زن و در نتیجه تاثیراتش را روی خواندن و ترجمه آیات قرآن کریم بررسی کند و ببیند که آیا تفاوت های واژگانی عمده ای میان این مترجمین وجود دارد یا نه. به این منظور، ترجمه 24 آیه از آیات قرآن کریم مورد بررسی مقایسه ای قرار ...
15 صفحه اولcontribution of setting to the study of characters and the main idea in e. brontes: wuthering heights and t. hardys: return of the native.
this thesis aims to adduce an unmitigated and comprehensive explication concerning the relationship of three significant elements of fiction: setting, chracter and theme. my research is basically placed on two outstanding novels of the 19th century: emily brontes wuthering heights and thomas hardys return of the native. my endeavour lies in studying the correlation among the three above-mention...
15 صفحه اولمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 38 شماره 1
صفحات 76- 86
تاریخ انتشار 2019-06
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
کلمات کلیدی برای این مقاله ارائه نشده است
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023