Journal: :Journal of the mechanical behavior of biomedical materials 2011
Miloš Janeček František Nový Josef Stráský Petr Harcuba Lothar Wagner

Ti-6Al-4V hour-glass shaped rotating beam specimens with duplex microstructure were processed by electric discharge machining (EDM). A comparatively high peak current of 29A was utilized in order to increase surface roughness for improved osteointegration. High cycle fatigue (HCF) tests were performed in rotating beam loading (R=-1) on these EDM specimens and results were compared with electrol...

2017
Chengsong Liu Daoxin Liu Xiaohua Zhang Shouming Yu Weidong Zhao

The effect of the ultrasonic surface rolling process (USRP) on the rotary bending fretting fatigue (FF) of Ti-6Al-4V alloy was investigated. The reason for the USRP's ability to improve the FF resistance of Ti-6Al-4V alloy was studied. The results revealed that the USRP induced a compressive residual stress field with a depth of 530 μm and a maximum residual stress of -930 MPa. Moreover, the su...

2008
A. Gutiérrez

In the present work, the oxide layers developed at elevated temperature on three vanadium-free titanium alloys, of interest as implant biomaterials, were studied by Rutherford backscattering spectroscopy, elastic recoil detection analysis, and scanning electron microscopy. The chemical composition of the alloys investigated, in wt%, was Ti–7Nb–6Al, Ti–13Nb–13Zr, and Ti–15Zr–4Nb. Upon oxidation ...

Journal: :Acta biomaterialia 2008
D Cáceres C Munuera C Ocal J A Jiménez A Gutiérrez M F López

The mechanical properties of the oxide layers developed at elevated temperature on three vanadium-free titanium alloys of interest for biomedical applications were investigated by means of the nanoindentation technique. The as-received alloys (Ti-13Nb-13Zr, Ti-15Zr-4Nb and Ti-7Nb-6Al) and their oxide scales formed by reaction with air at 750 degrees C for several oxidation times were analysed c...

Journal: :Journal of oral science 2011
Thanaphum Osathanon Kritchai Bespinyowong Mansuang Arksornnukit Hidekazu Takahashi Prasit Pavasant

There have been a number of attempts to modify the surface of dental implants to improve osseointegration. These modifications include alterations of surface chemistry and roughness. The purpose of this study was to examine the early response of human osteoblast-like cells placed on Ti-6Al-7Nb disks that had a similar grooved surface topography and three different levels of surface roughness (R...

Due to special properties such as low density, high strength and high corrosion resistance Ti-6Al-4V alloy has been used extensively in various industries, especially in the aerospace aspects. However the major problem of this alloy is its poor tribological properties under relatively high loads. In the present study, in order to improve the tribological properties of mentioned alloy, chromium ...

ژورنال: :صوت و ارتعاش 0
اسماعیل گنجه کارشناس ارشد مهندسی مواد دانشگاه صنعتی خواجه نصیرالدین طوسی حمید خرسند استادیار دانشکدة مهندسی مواد دانشگاه صنعتی خواجه نصیرالدین طوسی

آلیاژ ti-6al-4v در یک کوره اتمسفر کنترل توسط آلیاژ پرکننده آمورف 1228 stemet با ترکیب شیمیـایی (ti-27zr-14cu-13ni, wt%) لحیم شد. ابتدا کیفیت اتصالات لحیم توسط آزمون اولتراسونیک و با استفاده از روش اندازه گیری ضخامت کراتکرامر برانسون[i] ارزیابی شد. سپس تأثیر زمان و دماهای مختلف بر ریزساختار و خواص مکانیکی بررسی شد. بررسی ریزساختار توسط میکروسکوپ نوری، میکروسکوپ الکترونی روبشی[ii] و بررسی خواص مک...

ژورنال: :علوم و مهندسی سطح ایران 0

در این پژ‍وهش به بررسی تاثیر عملیات سطحی اصطکاکی اغتشاشی بر رفتار خوردگی آلیاژti-6al-4v  پرداخته شده است. برای این منظور، آزمون های پتانسیل مدار باز، پتانسیودینامیک و طیف سنجی امپدانس الکتروشیمیایی در محلول رینگر و دمای°c 37 انجام شد. نتایج آزمون های پلاریزاسیون نشان داد که آلیا‍ژ‍‍ ti-6al-4v قبل و بعد از عملیات اصطکاکی اغتشاشی بصورت خودبخودی رویین شده و تا پتانسیل 3 ولت (نسبت به الکترود کالومل...

ژورنال: مواد نوین 2015
محبوبه محمودی, محمدمهدی اسماعیلی

در این تحقیق، نانولایه کاربید تانتالوم با ضخامت 500 نانومتر بر روی سطح آلیاژ Ti-6Al-4V با روش رسوب دهی فیزیکی از فاز بخار با پرتو الکترونی به منظور اصلاح سطح زیرلایه، پوشش داده شد. با ارزیابی سختی سطح نمونه­ها، سختی سطح نمونه اصلاح شده با پوشش کاربید تانتالوم (Ti-6Al-4V/Ta2C) نسبت به نمونه بدون پوشش (Ti-6Al-4V) به عنوان شاهد از HV346 به HV640 افزایش یافت. هم­چنین با انجام آزمون خوردگی در محلول ...

2012
Shabnam Hosseini

Metallic biomaterials have essentially three fields of use; these are the artificial hip joints, screw, plates and nails for internal fixation of fractures, and dental implants. Any of these devices must support high mechanical load and resistance of material against breakage is essential. High mechanical properties are needed for structural efficiency of surgical and dental implants. But their...