Journal: :Acta odontologica latinoamericana : AOL 2009
Noé Orellana Robert Ramírez Miguel Roig Luís Giner Montse Mercade Fernando Durán Gerardo Herrera

The aim of this study was to compare the microtensile bond strength of three different total etch adhesives: XP Bond (Caulk-Dentsply) versus Excite (Ivoclar/Vivadent) and Prime & Bond NT (Caulk-Dentsply). Forty two (42) third human molars were cut to expose the dentinal surface. They were divided into three groups of 14 teeth (GI: XP Bond, G2: Excite, G3: Prime & Bond NT) and two groups of seve...

Journal: :Brazilian oral research 2013
Sheila Pestana Passos Rodrigo Othávio Assunção Souza Silvia Masae Araújo Michida Sandra Costa Zamboni Simone Helena Gonçalves de Oliveira

The aim of this study was to evaluate the effects of different light-curing units and resin cement curing types on the bond durability of a feldspathic ceramic bonded to dentin. The crowns of 40 human molars were sectioned, exposing the dentin. Forty ceramic blocks of VITA VM7 were produced according to the manufacturer's recommendations. The ceramic surface was etched with 10% hydrofluoric aci...

2013
Renato Roperto Mohamed Ghazy Omar El-Mowafy Igor J Pesun

Purpose: This study evaluated the influence of surface treatments on the microtensile bond strength between a glass fiber post surface and resin cements. Methods: Forth-five posts (Reforpost, Angelus, Londrina, PRBrazil) were assigned to three groups with different surface treatment: Group 1: No treatment and silane application only (G1); Group 2: immersion in 96% ethyl alcohol for 10 minutes f...

2015
Larissa Marinho AZEVEDO Leslie Carol CASAS-APAYCO Carlos Andres VILLAVICENCIO ESPINOZA Linda WANG Maria Fidela de Lima NAVARRO Maria Teresa ATTA

UNLABELLED Interface integrity can be maintained by setting the composite in a layering technique and using liners. OBJECTIVE The aim of this in vitro study was to verify the effect of resin-modified glass-ionomer cement (RMGIC) lining and composite layering technique on the bond strength of the dentin/resin adhesive interface of lateral walls of occlusal restorations. MATERIAL AND METHODS ...

2017
Marco Daniel Septimo Lanza Karina Kato Carneiro Alessandro Dourado José Bauer

This study evaluated microtensile bond strength (μTBS), degree of conversion, modulus of elasticity and ultramicrohardness of three etch-and-rinse adhesives systems. The materials evaluated were: Ambar (FGM), Optibond (Kerr) and Magic Bond (Vigodent). The degree of conversion was analyzed by FTIR/ATR. To evaluate bond strength (μTBS) in dentin, 15 teeth (n = 5) were restored and sliced to obtai...

2005
J. B. C. Meira R. Y. Ballester L. Driemeier

Recently the bond strength of composite resin to tooth has received attention from researchers of dental materials. Limitations imposed by the biological substrate, such as the size of the specimen, fostered the development of a tensile test with small dimensions. Due to the reduced size of the specimens, the test is called microtensile test. The specialized literature has not presented standar...

Journal: :journal of dentistry, tehran university of medical sciences 0
mina biria associate professor, department of pediatric dentistry, school of dentistry, shahid beheshti university of medical sciences, tehran, iran. amir ghasemi associate professor, preventive dentistry research center, research institute of dental science, department of restorative dentistry, dental school, shahid beheshti university of medical science, tehran, iran. hassan torabzadeh associate professor, iranian center for endodontic research, research institute of dental sciences, shahid beheshti university of medical sciences, tehran, iran. arash shisheeian post graduate student, department of prosthodontics, school of dentistry, shahid beheshti university of medical sciences, tehran, iran. alireza akbarzadeh baghban associate professor, department of basic sciences, faculty of rehabilitation sciences, shahid beheshti university of medical sciences, tehran, iran.

recently, self-etching fissure sealants have been introduced to reduce technical sensitivity; however, their efficacy should be assessed. the aim of this study was to assess of the microshear bond strength of self-etching and conventional fissure sealants.thirty non-carious third molars were randomly divided into three groups (n=10). microcylinders of concise fissure sealant were bonded to prep...

Journal: :Dental materials journal 2015
Shihchun Ting Afm Almas Chowdhury Feng Pan Jiale Fu Jihow Sun Shinichi Kakuda Shuhei Hoshika Yasuhiro Matsuda Takatsumi Ikeda Yasuko Nakaoki Shigeaki Abe Yasuhiro Yoshida Hidehiko Sano

The purpose of this study was to evaluate the effect of remaining dentin thickness (RDT) on the bond strength of current adhesive systems. Third molars were randomly allocated among four groups depending on the adhesive system used: Clearfil SE Bond ONE (SE1), G-Bond PLUS (GB), BeautiBond (BB), and Clearfil Mega Bond (MB). Bonded specimens were stored in water at 37°C for 24 h. Teeth were then ...

2017
Porntida Visuttiwattanakorn Kallaya Suputtamongkol Duangjai Angkoonsit Sunattha Kaewthong Piyanan Charoonanan

PURPOSE The objective of this study was to investigate the effect of surface treatments on microtensile bond strengths (MTBSs) of two types of indirect resin composites bonded to a conventional direct resin composite. MATERIALS AND METHODS Indirect resin composite blocks of Ceramage and SR Nexco were prepared in a plastic mold having a dimension of 10 × 10 × 4 mm. These composite blocks were ...

پایان نامه :وزارت علوم، تحقیقات و فناوری - دانشگاه صنعتی امیرکبیر(پلی تکنیک تهران) - دانشکده مهندسی عمران 1386

در این پژوهش تلاش شده است تا با انجام مشاهدات مستقیم آزمایشگاهی بر حدود تاثیرگذاری سه پارامت "سیکل های گرم وسرد شدن لوله" و "زبری سطح ورق فولاد" و همچنین "دامنه تغییرات دما" بر یک معیار مقاومتی مرتبط همچون مقاومت پیوستگی (bond strength) بین پوشش و فولاد تعیین گردد.

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید