نتایج جستجو برای: پالیش wear

تعداد نتایج: 26492  

2013
Roseline Meshramkar K Lekha Ramesh Nadiger

The aim of the review was to present the importance of tooth wear, etiology and its management in elderly patients. The success of rehabilitation of tooth wear in elderly depends up on finding the etiology, correct diagnosis, prevention method and its management. Recognition of the early signs of tooth wear could bring about timely prevention and improve the life span of teeth in elderly.

1998
D. M. Kennedy

This paper examines methods of assessing the wear resistance of coated and uncoated materials. Test equipment for sliding wear, erosion, impact and dynamic wear tests is discussed. Processes for measuring wear rates are highlighted and a simple procedure for conducting wear tests to simulate industrial wear problems is given. The wear test selected and the wear conditions encountered in real ap...

2013
A. Kawamura

Simultaneous measurements of the curves for wear versus distance, wear rate versus distance, and coefficient of friction versus distance were performed in situ to distinguish the transition from severe running-in wear to mild wear. The effects of the initial surface roughness on the severe running-in wear volume were investigated. Disk-on-plate friction and wear tests were carried out with SUS3...

2014
Biju Thomas

Tooth wear (attrition, erosion and abrasion) is perceived internationally as a growing problem .The loss of tooth substance at the cementoenamel junction because of causes other than dental caries has been identified as non-carious cervical lesions (NCCLs) or cervical wear. NCCLs can lead to hypersensitivity, plaque retention, pulpal involvement, root fracture and aesthetic problems. Hence stud...

2017
Saverio Affatato Maria Cristina Valigi Silvia Logozzo

The objective of this study was to examine total knee polyethylene inserts from in vitro simulation to evaluate and display-using a 3D optical scanner-wear patterns and wear rates of inserts exposed to wear by means of simulators. Various sets of tibial inserts have been reconstructed by using optical scanners. With this in mind, the wear behavior of fixed and mobile bearing polyethylene knee c...

Journal: :The Journal of bone and joint surgery. British volume 2001
J E Nevelos F Prudhommeaux M Hamadouche C Doyle E Ingham A Meunier A B Nevelos L Sedel J Fisher

We compared and quantified the modes of failure and patterns of wear of 11 Mittelmeier and 11 Ceraver-Ostal retrieved alumina-alumina hip prostheses with reference to the corresponding clinical and radiological histories. Macroscopic wear was assessed using a three-dimensional co-ordinate measuring machine. Talysurf contacting profilometry was used to measure surface roughness on a microscopic ...

Ameri, Hamideh, Moghadas, Mohammad gavad, Salehi, Amir, Sarabi, Nasrin,

Laboratory evaluation of composite wear resistance with and without occlusal index Dr. MJ. Moghadas * - Dr. N. Sarabi * - Dr. H. Ameri * - Dr. A. Salehi** *Assistant Professor of Operative Dentistry Dept., Faculty of Dentistry, Mashhad University of Medical Sciences. ** Dentist. Abstract Background and Aim: The polishing and finishing procedures may cause topographical changes and introduce sub...

Shahryar Pashaei, Soleyman Hosseinzadeh

Polyvinyl ester green composites were synthesized with walnut shell powder (WSP) by in-situ polymerization technique. The green composites have been evaluated for mechanical properties such as tensile strength, tensile modulus and hardness. Sliding wear loss, specific wear rate and coefficient of friction were investigated by using computerized pin-on–disc machine at normal applied loads of 20,...

Ebrahim Karamian Hassan Gheisari,

Most of the materials used in the industry of aero-engine components generally consist of titanium alloys. Advanced materials, because of their excellent combination of high specific strength, light weight and general corrosion resistance. In fact, chemical wear resistance of aero-engine alloy provides a serious challenge for cutting tool material during the machining process. The reduction in ...

E. Moayerifar Gh. Zirehpour R. Shoja Razavi

As the turbine industries need to manufacture turbine blades made of martensitic stainless steel AISI 420 with high toughness and wear resistance, local laser hardening has become more and more important. In this research, surface of the samples was initially hardened by high-power pulsed laser beam; then, optimum parameters of hardening were calculated and wear resistance of surface hardened s...