In this work, magnetic Ni nanowire arrays were ac-pulse electrodeposited into the anodic aluminum oxide (AAO) template fabricated by the common two-step anodization technique. The barrier layers at the  bottom of the pores were exponentially thinned in a non-equilibrium anodization process to 8, 12, 16 and 20 V. These were fabricated using the constant of 15 mA deposition current, 48 mS off-tim...

Journal: :journal of nanostructures 2015
z. haji jamali m. almasi kashi a. ramazani

nicu alloy nanowires arrays were embedded into the anodic aluminum oxide (aao) template by ac-pulse electrodeposition. different off-time were used in electrolyte with constant concentration of ni and cu and acidity of 3. the effect of deposition parameters on alloy contents was investigated by studying the microstructure and magnetic properties of as-deposited nicu alloy nanowires. atomic forc...

2009
Hai M. Duong Kei Ishikawa Jun Okawa Kazuaki Ogura Erik Einarsson Junichiro Shiomi Shigeo Maruyama

Arrays of vertically aligned single-walled carbon nanotubes (VASWNTs) were coated with thin films of Ti, Pd, Au, and Al by evaporative deposition. Scanning electron microcopy (SEM) showed the Ti and Pd coatings were continuous or quasi-continuous, while Au and Al agglomerated into discrete deposits on SWNT bundles. The mechanism of metal film formation on VASWNT arrays was studied by observing ...

2017
Emine Bakan Georg Mauer Yoo Jung Sohn Dietmar Koch

From the literature, it is known that due to their glass formation tendency, it is not possible to deposit fully-crystalline silicate coatings when the conventional atmospheric plasma spraying (APS) process is employed. In APS, rapid quenching of the sprayed material on the substrate facilitates the amorphous deposit formation, which shrinks when exposed to heat and forms pores and/or cracks. T...

2017
Zhiguo Wang Jibin Zhao Yuhui Zhao Hongyu Zhang Fan Shi

K465 superalloy with high titanium and aluminum contents was easy to crack during laser metal deposition. In this study, the crack-free sample of K465/Stellite-6 laminated material was formed by laser metal deposition shaping to control the cracking behaviour in laser metal deposition of K465 superalloy. The microstructure differences between the K465 superalloy with cracking and the laminated ...

Journal: :IOP Conference Series: Materials Science and Engineering 2013

Journal: :Materials Sciences and Applications 2013

Journal: :physica status solidi (RRL) – Rapid Research Letters 2019

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید