K. Zangeneh Madar and S. M. Monir Vaghefi,

In the present stady, thermochemical treatment in H2/NH3 atmosphere was used as a post-treatment for electroless Ni-P coatings on the AISI 4140 steel substrates. High phosphorus (9%) coatings with thicknesses of 2, 24 and 48 m were applied and the effects of the thermochemical treatment on the morphology, structural changes, roughness, hardness &#10&#10and wear resistance of coatings were studi...

2013
Atul Kulkarni Girish Joshi

In the present work Taguchi method is used to optimize cutting parameters during dry turning of AISI 304 austenitic stainless steel with AlTiCrN coated tool. The coating was deposited on fine-grained K-grade (ISO K-20) cemented carbide cutting insert using physical vapor deposition (PVD) technique. The turning parameters evaluated are cutting speed of 200 and 260 m/min, feed rate of 0.20 and 0....

2016
W. Pawlak K. J. Kubiak B. G. Wendler T. G. Mathia

A significant improvement of tribological properties on Ti-6Al-4V has been achieved by developed in this study multilayer treatment method for the titanium alloys. This treatment consists of an intermediate 2 μm thick TiCxNy layer which has been deposited by the reactive arc evaporation onto a diffusion hardened material with interstitial O or N atoms by glow discharge plasma in the atmosphere ...

2016
A. Sivaraman

The PVD techniques range over a wide variety of applications from decorative, to high temperature superconducting films. The thickness of the deposits can vary from angstroms to millimeters. A very large number of inorganic materials—metals, alloys, compounds, and mixtures—as well as some organic materials can be deposited using Physical vapour Deposition (PVD) technologies. Traditionally, the ...

2017
Elena Gracia-Escosa Ignacio García Juan J. de Damborenea Ana Conde

Boron steels are used in hot stamping process due to their good mechanical properties. During the stamping process, the dies are exposed to aggressive conditions including adhesive wear, abrasion, thermal stresses and fatigue. In the present work, QRO 90 and UNIMAX slid against 22MnB5 steel in four conditions: with and without hardening treatment and, with and without Al–10%Si coating, in order...

Journal: :The Journal of bone and joint surgery. British volume 1998
E W Morscher A Hefti U Aebi

One concern about the fixation of HA-coated implants is the possible disintegration of the surface, with the migration of HA granules into the joint space, producing third-body wear. We report a study of six revisions of HA-coated polyethylene RM cups at 9 to 14 years after successful primary arthroplasty. In all six hips, we found HA granules embedded in the articulating surface of the polyeth...

Journal: :Journal of Physics: Conference Series 2021

The work comparatively studies the wear kinetics of copper friction pairs with Chevrel phase-based coating (Cu-Mo-S) and without it in vacuum 1.5x10−3 Pa. is deposited on test pads by ion-plasma method. tribological investigations scheme were used "disk – coated pad". detected falling rate pair explained change adhesive mechanism to fatigue one.