نتایج جستجو برای: dentin bonding agents

تعداد نتایج: 409590  

Journal: :The journal of contemporary dental practice 2012
Pooran Samimi Mehrdad Barekatain Samaneh Alaei

INTRODUCTION The success of bonded restorations depends on effective bonding between restorative materials and tooth structure, and it prevents microleakage. New dentin bonding systems have been introduced which promotes this concept. The aim of this study was to compare the amount of microleakage between 'single bond' vs 'Prompt L-Pop' during different time periods. MATERIALS AND METHODS In ...

Journal: :American journal of dentistry 1988
C F Cox D Felton G Bergenholtz

The purpose of this study was to observe the pulpal response of bacterially infected cavities restored with either Gluma or Scotchbond. Cl V cavities (120) were distributed throughout the dentitions of five adult Macaca mulatta monkeys at intervals of 8 and 90 days. Each cavity was left open to the oral microflora for 48 hours to allow bacterial invasion of the remaining dentin. Six treatment g...

Journal: :journal of dentistry, tehran university of medical sciences 0
a. makarem professor, department of pediatric dentistry, school of dentistry, mashhad university of medical sci m. ebrahimi assistant professor, department of pediatric dentistry, school of dentistry, mashhad university of m m. talebi f. sadeghipour dentist

objective: considering the fact that several bonding agents are available in market, clinical evaluations are required to find the durability of the sealants after using bonding agents. the purpose of this study was to compare the durability of the fissure sealant after applying two kinds of dentin bonding materials, adhese and excite. materials and methods: in this clinical study sample group ...

Journal: :European journal of oral sciences 2016
Jae-Hoon Kim Geum-Jun Han Chang-Keun Kim Kyu-Hwan Oh Sung-No Chung Bae-Hyeock Chun Byeong-Hoon Cho

Non-thermal atmospheric pressure plasmas (NT-APPs) have been shown to improve the bond strength of resin composites to demineralized dentin surfaces. Based on a wet-bonding philosophy, it is believed that a rewetting procedure is necessary after treatment with NT-APP because of its air-drying effect. This study investigated the effect of 'plasma-drying' on the bond strength of an etch-and-rinse...

Journal: :Dental materials journal 2008
Masanori Hashimoto Shinichi Fujita Masayuki Kaga Yasutaka Yawaka

This study evaluated the effect of water on dentin substrate bonding of one-bottle self-etching adhesives. Dentin substrates were divided into two groups: wet and dry dentin. Wet dentin is the normal substrate for bond testing whereas dry dentin was dehydrated in a desiccator for 24 hours. Bonded dehydrated teeth were then divided into two subgroups: stored in water or in desiccator for 24 hour...

Haleh Heshmat, Mansoureh Emami Arjomand, Maryam Hoorizad Ganjkar, Mohammad Hossein Jahangiri, Mohammad Javad Kharazifard,

Background and Aim: Recurrent caries and low bond strength are the main causes of composite restorations failure. This study sought to assess the effect of chlorhexidine (CHX) on micro-shear bond strength (MSBS) to dentin of a fourth generation adhesive system and a universal bonding agent after aging. Materials and Methods: This in vitro study used 32 extracted third molars and 3-5mm thick de...

Journal: :Dental materials journal 2007
Mizuho Kusunoki Kazuo Itoh Yutaka Utsumi Hisashi Hisamitsu

The objective of this study was to evaluate the effects of triethylene glycol (TEG) and triethylene glycol monomethacrylate (TEGMA) solutions as dentin primers on dentin bonding. To this end, wall-to-wall polymerization contraction gap width of a resin composite in a cylindrical dentin cavity and shear bond strength to a flat dentin surface were measured. Dentin was pretreated with an experimen...

Journal: :Dental materials journal 2001
K K Chen Y Shono T Ogawa Y Kozono M Terashita

Comparative studies on resin-dentin bond strength and failure mode were performed between the conventional tensile test and the microtensile test with non-trimming small specimens, 1 x 1 mm in cross-section, for two brands of dentin bonding systems. The fracture surface of the conventional large specimen showed a catastrophic cohesive failure in dentin at its center and a lesser adhesive failur...

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید