Journal: :Crystals 2023

We have simulated a series of nanoindentation experiments on nanocrystalline tungsten specimens using combination molecular dynamics simulations and the embedded atom method potential. The research aimed to investigate impact grain size mechanical properties tungsten. Nanoindentation is technique used measure materials at small scale. In this study, researchers varied specimens, ranging from 7....

2016
Zhangwei Chen Nigel Brandon

The objectives of this study were to analyse the effect of inkjet 3-D printing parameters, particularly the splat overlap distance, for the fabrication of defect-free porous Al2O3 ceramic multilayers, and to correlate the resulting porosities with the mechanical properties measured using nanoindentation. An aqua-based alumina ink was used in this study to fabricate the multilayers on dense alum...

2016
Congrui Jin Donna M. Ebenstein

Nanoindentation testing of compliant materials has recently attracted substantial attention. However, nanoindentation is not readily applicable to softer materials, as numerous challenges remain to be overcome. One key concern is the significant effect of adhesion between the indenter tip and the sample, leading to larger contact areas and higher contact stiffness for a given applied force rela...

2014
Boris Polyakov Mikk Antsov Sergei Vlassov Leonid M Dorogin Mikk Vahtrus Roberts Zabels Sven Lange Rünno Lõhmus

The mechanical properties of thick-walled SiO2 nanotubes (NTs) prepared by a sol-gel method while using Ag nanowires (NWs) as templates were measured by using different methods. In situ scanning electron microscopy (SEM) cantilever beam bending tests were carried out by using a nanomanipulator equipped with a force sensor in order to investigate plasticity and flexural response of NTs. Nanoinde...

2017
Olha Shpotyuk Stanislaw Adamiak Elvira Bezvushko Jozef Cebulski Maryana Iskiv Oleh Shpotyuk Valentina Balitska

Light-curing volumetric shrinkage in dimethacrylate-based dental resin composites Dipol® is examined through comprehensive kinetics research employing nanoindentation measurements and nanoscale atomic-deficient study with lifetime spectroscopy of annihilating positrons. Photopolymerization kinetics determined through nanoindentation testing is shown to be described via single-exponential relaxa...

2006
Zehui Jiang Yan Yu Daochun Qin Ge Wang Bo Zhang Yuejin Fu

In situ imaging nanoindentation was used to characterize the mechanical properties of pure paint films on eight types of plywood-based flooring with different wear resistance. Correlation between the mechanical properties of paint films and the wear resistance of wood-based floorings was investigated. The average modulus of elasticity (MOE) and hardness of the paint film tested were 3.33–5.77 a...

2004
Fan Smith Harris Zaifeng. Fan

+Fan, ZF; *Smith, PA, +Harris,GF; [email protected] +Orthopaedic & Rehabilitation Engineering Center (OREC) Marquette University/Medical College of Wisconsin, Milwaukee, WI *Shriners Hospital for Children, Chicago, IL Introduction: Nanoindentation was used to characterize the intrinsic mechanical properties of bone tissue from eight (8) children with type III Osteogenesis Imperfecta (OI...

2017
Shih-Wei Liang Ren-Zheng Qiu Te-Hua Fang

The dynamic nanomechanical characteristics of Cu films with different grain boundaries under nanoindentation and scratch conditions were studied by molecular dynamics (MD) simulations. The type of grain boundary is the main factor in the control of the substrate atoms with respect to the size of dislocations since the existence of the grain boundary itself restricts the movement associated with...

2014
Jing Xu Surendra P. Shah

Investigation on the mechanical properties of cement-based materials at micron and submicron scales is important for understanding the overall performance, particularly of high-performance concrete (HPC). Due to low water-tocement ratio of HPC, a large amount of unhydrated cement grains remain in matrix, and a significant impact of the interface between C–S–H gel and cement grains on concrete b...

2006
B. Oommen K. J. Van Vliet

Scanning probe microscope-enabled nanoindentation is increasingly reported as a means to assess the mechanical properties of nanoscale, compliant material volumes such as polymeric films and bio-membranes. It has been demonstrated experimentally that the Hertzian contact model developed for linear elastic materials of semi-infinite thickness fails to accurately predict the nominal elastic modul...