آلیاژ ti-6al-4v در یک کوره اتمسفر کنترل توسط آلیاژ پرکننده آمورف 1228 stemet با ترکیب شیمیـایی (ti-27zr-14cu-13ni, wt%) لحیم شد. ابتدا کیفیت اتصالات لحیم توسط آزمون اولتراسونیک و با استفاده از روش اندازه گیری ضخامت کراتکرامر برانسون[i] ارزیابی شد. سپس تأثیر زمان و دماهای مختلف بر ریزساختار و خواص مکانیکی بررسی شد. بررسی ریزساختار توسط میکروسکوپ نوری، میکروسکوپ الکترونی روبشی[ii] و بررسی خواص مک...
Direct metal laser sintering (DMLS) is a selective laser melting (SLM) manufacturing process that can produce near net shape parts from metallic powders. A range of materials are suitable for SLM; they include various metals such as titanium, steel, aluminium, and cobalt-chrome alloys. This paper forms part of a research drive that aims to evaluate the material performance of the SLM-manufactur...
The applicability of irregular prealloyed Ti-6Al-4V powder for the fabrication of titanium products by pressing and sintering and its employment as a master alloy to obtain the Ti-3Al-2.5V alloy was studied. To this end, the starting powders were characterised by dilatometry, differential thermal analysis and XRD. Green samples were obtained by cold uniaxial pressing, and the evolution of the m...
Wire + Arc Additive Manufacturing (WAAM) is an advanced manufacturing technology by inexpensive Gas Tungsten Welding (GTAW) technology. Key microstructural features of the as-built WAAM alloy include large columnar β grains, grain boundary α colonies, and Heat Affected Zone (HAZ) banding, which generally leads to low ductility anisotropy. In this study, Ti–6Al–xV (x = 0, 2, 4) alloys were prepa...
In this research, the effects of parameters include tool rotational and traverse speeds were investigated on heat generation and material flow during friction stir welding of Ti-6Al-4V alloy with computational fluid dynamics (CFD) method. Simulation results showed that with increasing of tool rotational and decreasing tool traverse speed, the more frictional heat generates which causes formatio...
The present paper describes the results of tests on the influence of human saliva and its substitutes on tribological characteristics of implant materials on the example of the Ti-6Al-4V (a-Ti) titanium alloy. The saliva substitutes were prepared on the basis of pyrophosphates and mucins dissolved in saline buffer. The results of the presented tribological tests show that the values of the para...
The application of Ti-6Al-4V alloy or commercially pure titanium for additive manufacturing enables the fabrication of complex structural implants and patient-specific implant geometries. However, the difference in Young's modulus of α + β-phase Ti alloys compared to the human bone promotes stress-shielding effects in the implant-bone interphase. The aim of the present study is the mechanical c...
In this research, Ti-6Al-4V alloy was brazed with 410 stainless steel by three different filler metals as silver-base, nickel-base, and titanium-base alloys. In order to obtain optimum clearance, brazing was done in three different clearances of 0.02, 0.04 and 0.06 mm. Also, the strength and hardness of the brazing zone were investigated. The results of shear strength showed that the brazed ...