direct composite resin restorations are widely used and the impact of different storage temperatures on composites is not well understood. the purpose of this study was to evaluate the microtensile bond strength of composite to dentin after different pre-curing temperatures.occlusal surfaces of 44 human molars were ground with diamond burs under water coolant and polished with 600 grit silicon ...
Influence of adhesive polymerization mode on dentin bond strength of direct core foundation systems.
This study examined the influence of various adhesive systems on dentin bond strength of direct core foundation resins. Two commercially available direct core foundation resin systems and 2 adhesive polymerization modes were used. Facial bovine dentin surfaces were wet ground on 600-grit SiC paper. Dentin surfaces were treated according to the manufacturers' instructions and were light polymeri...
background: based on contradictory findings concerning the use of lasers for enamel etching, the purpose of this study was to investigate the shear bond strength of teeth prepared for bonding with er-yag laser etching and compare them with phosphoric acid etching. materials and methods: in this in vitro study forty – eight premolars, extracted for orthodontic purposes were randomly divided in t...
Objective: This study aimed to evaluate the suitability of one specific silorane-based composite for the application as a repair material for different substrates. Materials and methods: Truncated cones of composites fabricated and thermocycled for 6000 cycles to serve as a substrate were made of two commercially available dimethacrylate-based composites (DBC) (Filtek Supreme and Clearfil APX) ...
objective: this study evaluated the influence of storage time on micro-shear bond strength of two self-etching materials to enamel and dentin. materials and methods: human third molar teeth were sectioned to 1.5 mm thick beams and randomly divided into 2 groups. in group i, se bond and in group ii, tri-s bond was used to bond a composite rod (ap-x) to each treated surface. specimens were prepar...
The aim of this study was to evaluate the effects of sandblasting and different chemical bonding agents on shear bond strength of zirconia and conventional resin cement. In this study, 35 zirconia specimens were treated as follows: Group I: control; Group II: sandblasting; Group III: sandblasting + Monobond S; Group IV: sandblasting + Monobond Plus; Group V: sandblasting + Z-Prime Plus. The spe...
Adhesion promoting monomers for precious metals, 2,3-epithiopropyl methacrylate (EP1MA), 4,5-epithiopentyl methacrylate (EP3MA), 9,10-epithiodecyl methacrylate (EP8MA), 10,11-epithioundecyl methacrylate (EP9MA), 9,10-epithiodecyl 4-vinylbenzoate (EP8VB), 2,3-epithiocyclohexyl methacrylate (EPCHMA), and 3,4-epithiobutyl 2,2-bis(methacryloyloxymethyl)-propionate (EP2BMA), were used as surface tre...
Strong or low-barrier hydrogen bonds have often been proposed in proteins to explain enzyme catalysis and proton-transfer reactions. So far (1)H chemical shifts and scalar couplings have been used as the main NMR spectroscopic signatures for strong H-bonds. In this work, we report simultaneous measurements of (15)N and (1)H chemical shifts and N-H bond lengths by solid-state NMR in (15)N-labele...
introduction : this in vitro study was designed to evaluate the effect of smear layer removal on push-out bond strength of white mineral trioxide aggregate (wmta) and calcium-enriched mixture cement (cem). materials and methods: dentin discs with 3 mm thicknesses were divided into 4 groups ( n =15): group 1: irrigation of the canal with normal saline and filling with wmta; group 2: irrigation w...
objective: the objective of this study was to compare the tensile bond strength of metal brackets bonding to glazed ceramic surfaces using three various surface treatments. materials and methods: forty two glazed ceramic disks were assigned to three groups. in the first and second groups the specimens were etched with 9.5% hydrofluoric acid (hfa). subsequently in first group, ceramic primer and...