نتایج جستجو برای: interface shear strength
تعداد نتایج: 465856 فیلتر نتایج به سال:
background: as the use of different irrigants to eliminate residual debris and smear layer in the field of endodontic is unavoidable, by considering the effect of irrigants on the bond strength of resin composite restorations, this study was designed to evaluate the effect of a mixture of a tetracycline isomer, an acid, and a detergent (mtad) on the shear bond strength of two self-etch adhesive...
Bonding between laboratory light-cured composite and surface treated Au-Ag-Pd alloy was investigated using newly developed 4-META/MMA-TBB opaque resin. Shear bond strength after 20,000 thermocycles obtained from heated alloy with this method was 25.1 MPa. Ion-coated specimen showed 25.6 MPa after 50,000 thermocycles with decrease in bond strength being small. Ferric chloride treated specimen, h...
In this study accumulative roll bonding (ARB) process up to 8 Cycles (equivalent strain of 6.4) at ambient temperature was used in order to improve the mechanical properties of Commercial purity titanium (CP-Ti).Several experiment has been done and Mechanical properties of specimen has been discussed. For investigating optical microscope punching and hardness test were utilized. This is the fir...
In this study accumulative roll bonding (ARB) process up to 8 Cycles (equivalent strain of 6.4) at ambient temperature was used in order to improve the mechanical properties of Commercial purity titanium (CP-Ti).Several experiment has been done and Mechanical properties of specimen has been discussed. For investigating optical microscope punching and hardness test were utilized. This is the fir...
geotechnical investigations of waste fills are rarely undertaken, and consequently the geotechnical community has little knowledge of their engineering properties. in this study, a geotechnical testing program was conducted to evaluate the engineering properties of old municipal solid waste sampled in whamyung msw landfill site, busan, korea. the conducted tests included water content, specific...
The purpose of this study was to compare side-by-side two different titanium screw-type implants in the maxillae of miniature pigs. The test implants had a machined and acid-etched surface (Osseotite) whereas the control implants were sandblasted and acid-etched (SLA). After 4, 8, and 12 weeks of healing, removal torque testing was performed to evaluate the shear strength of the bone-implant in...
The degree of adherence between two bituminous layers can be assessed from shear tests carried out at constant displacement speed, which allow the strength and stiffness interface to b...
نمودار تعداد نتایج جستجو در هر سال