Polysulfone-based composite materials filled with artificial, natural, or thermally expanded graphite have been investigated. Composite filling degrees between 30 and 70 wt.% were prepared using solution technology. High levels fillers allowed for the achievement of thermal conductivity 7.35 W/m · K electrical 52.9 S/cm. The use natural has found to greatest impact on characteristics, while dis...