Abstract The cause of a rare cracking failure accident the polyethylene (PE) anti-corrosion layers pipeline is analyzed and determined. properties PE raw materials were detected according to standard, micro-morphology was characterized by scanning electron microscope (SEM). storage modulus loss at range -100~40 °C tested dynamic mechanical analysis (DMA), stress low temperature (-40 °C) calcula...